MP35N Cobalt Alloy (ASTM F-562, ISO 5832-6)
MP35N Cobalt Alloy (ASTM F-562, ISO 5832-6)
MP35N (UNS R30035, ASTM F562, ISO 5832-6) yog nickel-cobalt-raws li austenitic alloy nrog cov ntsiab lus cobalt ntawm kwv yees li 35%. Raws li ASTM F562 thiab ISO 5832-6 tus qauv, MP35N tau pom meej meej tias yog wrought cobalt-nickel-chromium-molybdenum alloy rau kev cog hniav; nws yog tsim tshwj xeeb rau kev cog qoob loo rau tib neeg lub sijhawm ntev, ua tau raws li cov kev cai nruj rau biocompatibility, purity, thiab qaug zog.
Cov ntaub ntawv pov thawj ntawm cov khoom siv feem ntau sau ASTM F562, ISO 5832-6, thiab BS 7252-6 sab-los ntawm-sab ua pov thawj ntawm cov khoom siv kho mob-qib kev tsim nyog.
Rau cov khoom siv implantable, qhov no qhia txog cov hauv qab no:
Kev pib qaug zog tawg: Cov khoom nyuaj ua raws li cov ntsiab lus kev ntxhov siab, ua rau cov kab nrib pleb nyob rau hauv ntev - lub sij hawm pulsatile loading thiab tej zaum yuav ua rau tsis ua hauj lwm ntxov ntawm cov khoom siv xws li pacemaker leads.
Kev puas tsuaj: Thaum lub caij txias txias, cov khoom no tuaj yeem khawb qhov tuag, ua rau muaj qhov tsis xws luag ntawm cov hlau uas ua rau muaj kev cuam tshuam ntxiv rau kev ua haujlwm qaug zog.
Yog li ntawd, tiag tiag siab -kev ntseeg siab kho mob- qib MP35N yog tsim nrog titanium thiab nitrogen qib khaws cia zoo hauv qab qhov siab tshaj plaws uas tau teev tseg los ntawm cov qauv. Patents qhia meej meej tias cov khoom kho mob zoo tshaj - qib cov khoom lag luam tuaj yeem tswj cov qib titanium qis dua 0.01%- lossis txawm tias qis li 0.001%- yog li inhibiting tsim cov teeb meem cuam tshuam ntawm qhov chaw.
Dimensions thiab Profiles them los ntawm Core Standard
Bars-Cov khoom nrog puag ncig, duab plaub, lossis lwm yam duab, xa ncaj nraim thiab txiav mus rau qhov ntev.
Fine Wire-Cov khoom uas muaj puag ncig, duab plaub, lossis lwm yam duab uas muaj qhov sib txawv ntawm tus ntoo khaub lig- ntu raws lawv qhov ntev tag nrho, nrog txoj kab uas hla lossis tuab tsawg dua 1.60 hli [0.063 nyob rau hauv.], muab rau hauv coils, ntawm spools, lossis hauv lwm cov ntawv ntim raws li tau teev tseg.
Hlau-Cov khoom uas muaj puag ncig, duab plaub, lossis lwm cov duab sib txawv uas muaj cov ntoo khaub lig zoo ib yam - ntu raws lawv qhov ntev, nrog txoj kab uas hla lossis tuab tsawg dua 4.76 hli [0.1875 nyob rau hauv.], muab rau hauv cov coils, ntawm spools, lossis lwm cov ntawv ntim raws li tau teev tseg.
tshuaj muaj pes tsawg leeg
ASTM F-562 Cov Lus Qhia Tshwj Xeeb
|
Element
|
min
|
max |
| C | -- | 0.025 |
| Mn | -- | 0.15 |
| Si | -- | 0.15 |
| P | -- | 0.015 |
| S | -- | 0.010 |
| Cr | 19.0 | 21.0 |
| Ni | 33.0 | 37.0 |
| Mo | 9.0 | 10.5 |
| Fe | -- | 1.0 |
| Ti | -- | 1.0 |
| B | -- | 0.015 |
| Co | Tshuav |
Mechanical Properties (Bar Products)
|
Qhov xwm txheej
|
Tensile zog
MPa [psi]
|
Yield zog (0.2% Offset)
MPa [psi]
|
Elongation
min,%
|
Kev txo qis hauv cheeb tsam
min,%
|
|
Kev daws -annealed
|
793 to 1069 [{2}} rau 155 000]
|
241 txog 586 [{2}} rau 85 000]
|
50.0 | 65.0 |
|
Txias- ua haujlwm
nruab nrab nyuaj
|
1000 [145 000] min.
|
655 [{1}}] feeb.
|
20.0 | 60.0 |
|
nyuaj
|
1207 [{1}}] min. |
1000 [145 000] min.
|
10.0 | 50.0 |
|
Txias- ua haujlwm thiab hnub nyoog
|
1793 [260 000] min.
|
1586 [230 000] min. | 8.0 | 35.0 |
Mechanical Properties-Cov khoom siv hlau (d Ntau dua lossis sib npaug li 1.6 hli [0.063 nyob rau hauv.])
|
Qhov xwm txheej
|
Tensile zog
MPa [psi]
|
Yield zog (0.2% Offset)
MPa [psi]
|
Elongation
min,%
|
Kev txo qis hauv cheeb tsam
min,%
|
| Kev daws -annealed |
793 to 1069 [{2}} rau 155 000]
|
241 txog 586 [{2}} rau 85 000]
|
50.0 | 65.0 |
|
Txias- ua haujlwm
nruab nrab nyuaj
|
1000 [145 000] min.
|
655 [{1}}] feeb.
|
20.0 | 60.0 |
| nyuaj |
1207 [{1}}] min.
|
1000 [145 000] min.
|
10.0 | 50.0 |
| Txias- ua haujlwm thiab hnub nyoog |
1793 [260 000] min.
|
1586 [230 000] min.
|
8.0 | 35.0 |
Mechanical Properties-Zoo Hlau (d < 1.6 mm [0.063 nyob rau hauv.])
|
Txoj kab uas hla, mm [hauv.]
|
Annealed
|
|
|
Tensile zog,
MPapsi]
|
Elongation
min,%
|
|
|
<1.600 to 1.473
[<0.063 to 0.058]
|
827-1034 Ib
[120 000 rau 150 000]
|
40.0 |
|
<1.473 to 0.864
[<0.058 to 0.034]
|
862 rau 1069
[125 000 rau 155 000]
|
40.0 |
|
<0.864 to 0.406
[<0.034 to 0.016]
|
931-1138 Ib
[135 000 rau 165 000]
|
40.0 |
|
<0.406 to 0.0762
[<0.016 to 0.003]
|
1000-1207 Nws
[145 000 rau 175 000]
|
30.0 |
|
<0.0762 to 0.0508
[<0.003 to 0.002]
|
1034-1310 Nws
[150 000 rau 190 000]
|
30.0 |
|
<0.0508
[<0.002]
|
1172-1448 Ib
[170 000 rau 210 000]
|
25.0 |
| Txoj kab uas hla, mm [hauv.] |
Txias-Ua haujlwm
|
|||
|
Nyuaj
|
Caij nplooj ntoos hlav
|
|||
|
Tensile zog,
MPa [psi]
|
Elongation
min,%
|
Tensile zog,
MPa [psi]
|
Elongation
min,%
|
|
|
<1.600 to 1.473
[<0.063 to 0.058]
|
1655-1862 : kuv
[240 000 rau 270 000]
|
2.0 |
1862 rau 2068
[270 000 rau 300 000]
|
2.0 |
|
<1.473 to 0.864
[<0.058 to 0.034]
|
1689-1896 : kuv
[245 000 rau 275 000]
|
2.0 |
1896-2103 Nws
[275 000 rau 305 000]
|
2.0 |
|
<0.864 to 0.406
[<0.034 to 0.016]
|
Xyoo 1758 txog 1965
[255 000 rau 285 000]
|
2.0 |
Xyoo 1965-2172
[285 000 rau 315 000]
|
2.0 |
|
<0.406 to 0.0762
[<0.016 to 0.003]
|
1827-2034 Nws
[265 000 rau 295 000]
|
2.0 |
2034-2241 Ib
[295 000 rau 325 000]
|
2.0 |
|
<0.0762 to 0.0508
[<0.003 to 0.002]
|
1896-2103 Nws
[275 000 rau 305 000
|
2.0 |
2103-2310 Nws
[305 000 rau 335 000]
|
2.0 |
|
<0.0508
[<0.002]
|
Xyoo 1999-2275
[290 000 rau 330 000]
|
1.8 |
2206-2482 Ib
[320 000 rau 360 000]
|
1.8 |
Cov ntsiab lus tseem ceeb ua haujlwm
Machining MP35N (raws li ASTM F562 / ISO 5832-6 tus qauv) yog qhov nyuaj vim nws ua haujlwm nrawm heev - hardening npaum li cas - peb mus rau tsib npaug ntawm 316L stainless hlau - ua rau nws nyuaj -to-machine superalal Machining cov tswv yim yuav tsum tau ua raws li cov khoom siv thaum lub sijhawm ua haujlwm.
Machining nyob rau hauv qhov kev daws teeb meem -Kho (Annealed) Xeev
Thaum MP35N ua tiav nws lub zog siab kawg los ntawm kev sib xyaw ua haujlwm txias thiab kev laus, cov khoom siv los ua nyuaj heev hauv cov neeg laus (txog 45-55 HRC). Pa machining yog qhov tsis yooj yim sua nyob rau theem no, tawm hauv kev sib tsoo lossis Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob (EDM) tsuas yog kev xaiv siv tau.
Cov kev pom zoo ua haujlwm yog: Ua kom tiav cov khoom lag luam lossis cov raj khoob hauv cov tshuaj - kho (annealed) lub xeev (hardness approx. 25-32 HRC) → Ua kom tiav tag nrho cov roughing thiab semi- ua tiav cov haujlwm → Ua qhov kawg kev laus kom ua tiav lub zog xav tau. Kev yuav khoom ua ntej- hnub nyoog Tshuag yuav tsum tsuas yog txiav txim siab yog tias qhov yuav tsum tau muaj qhov tseeb thiab tsis tuaj yeem ua rau deformation thaum laus; Nyob rau hauv cov ntaub ntawv no, machining pub thiab cov txheej txheem tsis yuav tsum tau npaj nyias.
Txiav Parameters (Siv rau kev xa hauv qhov kev daws teeb meem-Thiab Xeev)
Thaum txiav hauv kev daws teeb meem-kho lub xeev, txoj hauv kev "tsawg ceev, siab pub, thiab txiav tob" yog qhov tseem ceeb los tiv thaiv lub cuab yeej los ntawm kev sib tsoo tawm tsam kev ua haujlwm- txheej tawv tawv dua li txiav los ntawm nws:
Cov cuab yeej xaiv: cov cuab yeej carbide (K- qib lossis PVD-coated) yuav tsum tau siv; kev siv siab - steel ceev (HSS) yog txwv tsis pub.

Paub meej cov khoom daim ntawv thiab xwm txheej
Ua ntej muab cov lus hais, peb yuav tham txog cov kev qhia tshwj xeeb hauv qab no nrog koj:
- Daim ntawv: Round bar, tiaj bar, hlau, los yog forging?
- Dimensions: Diameter/Sab Length, Length
- Qhov xwm txheej: Annealed (mos) lossis Txias -ua haujlwm / Hnub nyoog (nyuaj)?
- Nto tiav: Tig, av, pickled, lossis polished?
- Kev kho cua sov yuav tsum tau ua: Tus neeg muag khoom puas yuav tsum ua haujlwm txias thiab kev laus kho ua ntej xa khoom?
Lork Group
Kev Lag Luam Kev Lag Luam