Tom ntej: Inconel X750 Nickel Alloy Bars (UNS N07750)

Inconel X-750 bar Tshuag tau tsim tshwj xeeb los tiv thaiv qhov chaw huab cua. Peb cov hlau nplaum yog tsim nyob rau hauv nruj raws li cov qauv kev lag luam, ua kom cov khoom zoo tshaj plaws purity, uniformity, thiab ua tau zoo ib yam.
Nyob rau hauv aerospace cav thiab roj turbine sectors, peb X-750 alloy bar yog aptly lub npe hu ua "700-Degree Timekeeper." Nws tus nqi tseeb tsis yog nyob rau hauv nws lub peev xwm los tiv taus qhov kub thiab txias rau lub sijhawm luv luv, tab sis nyob rau hauv nws qhov tshwj xeeb tsis kam ua kom qeeb deformation (creep) thiab kev ua haujlwm tsis zoo nyob rau hauv qhov tseem ceeb ntawm 650℃txog 750℃qhov kub thiab txias - yog li ua kom ntseeg tau tias kev ua haujlwm ntawm cov khoom tseem ceeb tshaj kaum tawm txhiab teev. Xaiv cov khoom siv no txhais tau tias ua kom ruaj khov rau lub sijhawm ntev thiab kev cia siab rau kev ua haujlwm nyob rau hauv kev ua haujlwm hnyav.
Cov khoom siv no yog tsim los rau cov ntawv thov uas xav tau qib siab tshaj plaws, suav nrog turbine Cheebtsam rau aero- cav, bolts thiab springs rau roj turbines, siab - kub fasteners rau nuclear fais fab nroj tsuag, thiab thrust chambers rau foob pob ua ntxaij cav.
Cov ntaub ntawv siv
Inconel X-750 bars muaj nyob rau hauv ntau yam kev qhia tshwj xeeb, feem ntau muab faib ua ob hom: kub- dov / forged thiab txias-draw / hauv av.
Precision txias- rub / hauv av tuav: Ø2mm - Ø50mm (tsim rau kev siv tshuab tshuab tsis siv neeg)
Kub- dov / forged tuav: Ø50mm - Ø300mm+ (rau loj forgings lossis machining preforms)
Nqe Reference
Bars tuaj yeem muab tau rau hauv forged, kub- dov, tshuaj- kho, lossis txias- cov xwm txheej kos; tus nqi thiab cov yam ntxwv ua tau zoo sib txawv nyob ntawm qhov xwm txheej. Tus nqi dav dav peb tuaj yeem muab tau yog $ 75 - $ 145 ib kg.
Tus nqi siab teeb meem
Thaum peb hais tus nqi rau Inconel X750 nickel alloy tuav, feem ntau cov neeg siv khoom yuav hais tias, "Tus nqi no siab dhau lawm." Qee tus txawm ntshai los ntawm tus nqi siab thiab tsis txhob tiv tauj peb ntxiv.
Tab sis peb cov lus teb yog:
"Hais lus ncaj ncees, cov khoom siv thiab cov nqi tsim khoom ntawm X-750 feem ntau yuav yog ob peb zaug ntawm cov khoom siv kub kub zoo tib yam ($ 30- $ 50 / kg). Nws kim vim li cas, thiab nws tseem yog cov khoom tsis tshua muaj txawm tias cov khoom siv nce nqi."
Txawm li cas los xij, peb thov kom koj xav txog peb cov nqi no los ntawm kev pom zoo:
X-750 yog nag lossis daus-hardening alloy; tsis zoo li cov qauv stainless hlau, nws tsis yog "npaj-rau-siv" thaum yuav khoom thiab xav tau kev kho cua sov kom ua tiav nws cov khoom ua tau zoo.
Kev daws thiab kev laus kev kho mob: Cov khoom xav tau kev kho mob ntawm qhov kub thiab txias ua raws li kev laus kom precipitate 'theem ntxiv dag zog; Cov txheej txheem kev kho cua sov no siv lub sijhawm thiab lub zog ntawm lub cub tawg tseem ceeb.
Nyuaj rau lub tshuab: Tom qab muaj hnub nyoog- hardening, X-750 nthuav tawm hardness siab heev, ua rau machining nyuaj dua nrog 304 stainless hlau; Qhov no ua rau cov cuab yeej hnav sai thiab ua haujlwm tsis zoo.
Dimensional kho: Deformation yuav tshwm sim thaum lub sij hawm kho cua sov, yuav tsum tau ntxiv straightening los yog tiav cov txheej txheem.
Thaum kawg, peb yuav nthuav qhia koj nrog Lork Group's "toolbox": ib daim ntawv sau "X-750 Machining and Heat Treatment Guide," ib "Hloov Siab-Tsev Cov Ntaub Ntawv Kub" thiab cov qauv (yog tias muaj cov qauv tsim nyog). Tsis tas li ntawd, peb muab cov ntaub ntawv thov kev kawm (de-sensitized) ntawm cov roj turbine khi pas nrig rau koj siv.
Tshuaj muaj pes tsawg leeg
|
Cov ntsiab lus |
Cov ntsiab lus (%) |
|
S/C/Si/Cu |
cov lej |
|
Al |
0.40%~1.00% |
|
Co |
Tsawg dua lossis sib npaug li 1.00% |
|
Fe |
5.0%~9.0% |
|
Ni |
Ntau dua lossis sib npaug li 70.0% |
|
Mn |
Tsawg dua lossis sib npaug li 1.00% |
|
Ti |
2.25%~2.75% |
|
Nb+Ta |
0.70%~1.20% |
|
Cr |
14.0%~17.0% |
Tiv tauj peb rau Inconel X-750 spectrometer kuaj video
Email: [susan@lorkgroup.com]
WhatsApp: [+ 86 199 37075488]
Mechanical Composition
Thaum tham txog Inconel X-750, cov ntaub ntawv kub siab yuav tsum tau tshuaj xyuas. Qhov no yog nyob rau hauv cov txheej txheem kev laus.
|
Mob & Loj |
Tensile zog |
Yield zog |
Elongation |
Kev txo qis ntawm cheeb tsam |
Hardness |
|
MPa, min |
MPa, min |
%, min |
%, min |
HB |
|
|
Kev daws ntawm 2100℃F (1149 degree) + stabilize + nag lossis daus harden |
965 |
620 |
8 |
... |
262 nqi |
|
Kev daws ntawm 1800℃F (982 degree) + nag lossis daus harden / Mus txog 63.5mm, tshwj xeeb |
1170 |
790 |
18 |
18 |
302-363 |
|
Kev daws ntawm 1800℃F (982 degree) + nag lossis daus harden / 63.5 txog 101.6mm, tshwj xeeb |
1170 |
790 |
15 |
15 |
302-363 |
|
Kev daws anneal ntawm 2000℃F (1093 degree) + nag lossis daus harden |
1103-1276 |
689-896 |
20 |
20 |
267-363 |
Peb muab - cov ntaub ntawv ntsuas kub ua haujlwm rau peb cov ntaub ntawv, uas ua haujlwm ncaj qha rau koj tus qauv tsim.
Kev Qhia Txog Kev Muag Khoom thiab Kev Tsim Khoom
Thaum yuav X-750 alloy,70% ntawm tus nqi mus rau kev tsim khoom. Peb tsom los ua koj "kev kho cua sov navigator," daws koj daim ntawv thov kev sib tw rau aero engines thiab industrial turbines.
1. Cov Lus Qhia Txog Kev Muag Khoom:
"Kuv xav kom koj qhia meej rau hauv koj cov ntaub ntawv qhia kev thiab nug:Inconel X-750 (UNS N07750) ua raws li cov qauv tshwj xeeb; txoj kab uas hla, qhov ntev, thiab qhov ntau tau teev tseg, thiab qhov kev xa khoom yog kev daws teeb meem thiab hnub nyoog (piv txwv li, AH mob).Tsis txhob cia li yuav 'kev daws- kho'! Nws qhov kev ua tau zoo yog nyob ntawm kev kho cua sov kom raug, thiab lub luag haujlwm no yuav tsum tau ua los ntawm cov chaw tsim khoom. Peb tuaj yeem muab ntau yam khoom los ntawm forgings mus rau cov khoom tiav. "
2. Cov ntsiab lus tseem ceeb hauv Machining thiab kev kho cua sov (Peb tus nqi tseem ceeb-Cov ntsiab lus ntxiv):
"Muaj peb txoj haujlwm tseem ceeb uas txiav txim siab ua tiav lossis tsis ua tiav, uas peb pab peb cov neeg tau txais kev zam:
- 'Kev laus' tsis yog ib qho - cov txheej txheem, tab sis ob - cov txheej txheem:Tus qauv'AH condition'yog'kev laus nruab nrab ntawm 845℃+ kev laus kawg ntawm 705 degree'. Ob kauj ruam yog qhov tseem ceeb; qhov kub thiab lub sijhawm yuav tsum yog qhov tseeb. Muaj ntau qhov kev ua haujlwm tsis zoo tshwm sim los ntawm qhov no.
- Welding yog ib qho haujlwm tseem ceeb:X-750 tuaj yeem welded, tab sis aua tiav kev kho mob ntxiv rau ob- txheej txheem kev laus yog qhov tseem ceeb tom qab vuam; txwv tsis pub, lub tshav kub- thaj tsam cuam tshuam yuav dhau los ua qhov tsis muaj zog hauv kev ua haujlwm. Peb pom zoo kom tsis txhob welding nyob rau hauv tus tsim.
- Machining yuav tsum tau ua tib zoo saib xyuas kom meej:Cov khoom no muaj kuab heev thiab ua haujlwm - hardens sai. Cov cuab yeej ntse carbide, kev txiav qis qis, siab pub tus nqi, thiab cov dej txias txaus yog tsim nyog. Peb muaj cov ntaub ntawv ntawm machining tsis uas peb tuaj yeem qhia rau koj cov nroj tsuag machining.
3. Muab ob npaug rau Kev Ntsuam Xyuas Zoo:
"Peb muab cov ntaub ntawv AMS ua tiav nrog rau tus lej ntawm lub tshuab hluav taws xob rau txhua pawg. Qhov no los ntawm peb tus qauv -raws li kev soj ntsuam saum npoo, tshuaj lom neeg muaj pes tsawg leeg, kuaj cov cuab yeej siv tshuab, thiab lwm yam, raws li cov khoom tiav. Peb kuj khaws cov qauv, tshuaj xyuas cov duab, thiab cov yeeb yaj duab rau kev taug qab.
- Incoming PMI (spectral) pov thawj:Tsom ntsoov rau kev tshuaj xyuas cov txhuas (Al) thiab titanium (Ti) cov ntsiab lus hauv Inconel X-750 nickel alloy pas nrig. "Cov ntsiab lus.
- Thib peb - tog siab - ntsuas qhov ntsuas kub ua haujlwm(rau thawj tsab xov xwm lossis cov khoom tseem ceeb): Cov qauv raug txiav thiab xa mus rau ib lub tsev kawm ntawv muaj cai xws li Beijing Institute of Aeronautical Materials rau 'siab-kub durability test'. Txawm hais tias qhov no yog lub sij hawm-siv thiab kim, nws yog 'qhov kawg txiav txim' los xyuas seb cov khoom batch ua raws li cov ntaub ntawv thiab xyuas kom meej tias koj tus qauv tsim tsis muaj qhov tsis zoo. Peb tuaj yeem pab nrog kev sim.
Ntim & Shipping

Cim npe nrov: Inconel X750, Nickel Alloy Bars, UNS N07750, AMS 5667, Tuam Tshoj inconel alloy manufacturers, hoobkas