Ti-6Al-2Zr-1Mo-1V Titanium Alloy (TA15)

Ti-6Al-2Zr-1Mo-1V Titanium Alloy (TA15)

Lork Group yog tus neeg muag khoom thoob ntiaj teb uas ntseeg siab ntawm Ti-6Al-2Zr-1Mo-1V titanium alloy, ze-alpha titanium alloy muaj npe nrov rau nws lub zog kub kub, kev nkag siab zoo heev, thiab zoo dua weldability. Zoo tagnrho rau aerospace, marine, thiab cov ntawv thov kev lag luam, peb cov qib premium-qib alloy ua kom ruaj khov thiab ua haujlwm tau zoo hauv qhov chaw huab cua.
Xa kev nug

Ti-6Al-2Zr-1Mo-1V (TA15) yog ze-alpha titanium alloy nrog zoo kub-kub lub zog, nkag tsis kam, thiab weldability, ua rau nws haum rau aerospace thiab industrial daim ntaub ntawv.

 

Tshuaj muaj pes tsawg leeg

 

Khoom siv

TSI 15

 

tshuaj muaj pes tsawg leeg

Fe

C

Si

Mo

N

V

Zr

Al

H

O

Ti:

Tsawg dua lossis sib npaug li 0.25

Tsawg dua lossis sib npaug li 0.08

Tsawg dua los yog sib npaug li 0.15

0.5-2

Tsawg dua los yog sib npaug li 0.05

0.8-2.5

1.5-2.5

5.5-7.1

Tsawg dua lossis sib npaug li 0.015

Tsawg dua los yog sib npaug li 0.15

paj ntaub

 

 

Cov yam ntxwv tseem ceeb

  • Thermal stability

    Khaws lub zog thiab oxidation tsis kam ntawm 400-500 degree.

  • Corrosion Resistance

    Zoo tiv thaiv oxidizing ib puag ncig thiab dej ntsev corrosion.

  • Weldability & Processability

    Yuav welded los ntawm TIG (GTAW), laser, los yog electron beam txoj kev.

    Kub- ua haujlwm (forging, dov) ntawm 850-950℃yog qhov zoo.

  • Kev kho cua sov

    Annealing: 700-800℃(cua txias) kom txo tau kev ntxhov siab thiab txhim kho ductility.

    Kev Kho Mob + Kev laus (STA): Kev xaiv rau lub zog siab dua (piv txwv li, 950℃quenching + 500-600℃aging).

  • Daim ntawv thov

    Aerospace: Compressor hniav, cav casings (qhov twg Ti-6Al-4V qhov kub txwv yog tshaj).

    Marine: submarine Cheebtsam, nkoj hulls.

    Kev lag luam: High-kub fasteners, siab hlab ntsha.

 

Vim li cas thiaj xaiv Lork Group's Ti-6Al-2Zr-1Mo-1V Alloy?

 

  • Siab -Kev Ua Haujlwm Kub - ruaj khov mus txog 500℃(932℃F), ua haujlwm zoo dua Ti-6Al-4V.
  • Superior Creep Resistance - Txhim kho los ntawm zirconium (Zr) thiab molybdenum (Mo) ntxiv.
  • Zoo Corrosion Resistance - Zoo tagnrho rau kev siv marine, tshuaj, thiab aerospace.
  • Machinable & Weldable - Tau tshaj TIG, laser, thiab electron beam vuam.
  • Custom Solutions - Muaj nyob rau hauv ingots, tuav, nplooj ntawv, thiab forged Cheebtsam.

 

Email:susan@lorkgroup.com
WhatsApp pawg:+86 19937075488

 

Hu rau tam sim no

Cim npe nrov: TA15 Titanium Alloy Bar, TA15 Ti bar, Ti-6.5Al-2Zr-1Mo-1V, Ti-6Al-2Zr-1Mo-1V, Nyob ze- Titanium Alloy, High-Aluminium Sib npaug Titanium Alloy, Ti-6Al-2Zr-1Mo-1V

Xa kev nug