Kev Kho Mob Qib Stainless Hlau Rex 734 (1.4472)

Kev Kho Mob Qib Stainless Hlau Rex 734 (1.4472)

Lork Group yog lub ntiaj teb ua lag luam xa tawm thiab xa khoom ntawm Kev Kho Mob Qib Stainless Hlau Rex 734 (1.4472), qib siab -kev ua tau zoo alloy tshwj xeeb tsim rau kev phais, kho hniav, thiab cov cuab yeej siv kho mob. Thov cov qauv dawb & sib tw nqe lus hnub no!
Xa kev nug

 

Kev kho mob qib stainless hlau Rex 734 / 1.4472 yog implant alloy nrog siab xav tau raws li kev tiv thaiv corrosion thiab qaug zog. No High-Nitrogen stainless hlau muaj zog tensile zoo dua, hnav tsis kam, tsis kam rau pitting thiab crevice corrosion dua li qib 316LVM.

 

Tau los ntawm slag remelting, qib no tsis muaj ferrite thiab kev huv huv ntawm nws cov microstructure ua rau nws tsis yog -magnetic thiab biocompatible nrog tib neeg cov ntaub so ntswg. Cov hlau tsis muaj steel hlau no yog siv rau hauv kev tsim khoom hnyav- siv orthopedic implants thiab osteosynthesis li, xws li nyias nyias los yog siab -mobility prosthesis.

Medical Grade Stainl rex 734 bar

 

Cov teb tseem ceeb ntawm kev siv stainless hlau REX-734

 

Kev tsim cov pob txha phais - hloov rau lub duav, lub hauv caug, lub xub pwg nyom, pob txha- rau tes thiab rau cov khoom siv rau osteosynthesis.

 

Lork Group muab Kev Kho Mob Qib Stainless Hlau Rex 734 / 1.4472 round tuav uas ua raws li cov lus qhia hauv qab no thiab qhov ntev. Tiv tauj peb rau cov qauv dawb thiab cov lus hais.

Hu rau tam sim no

 

Normes

  • ASTM 1586, UAS 1586
  • TS EN ISO 5832-9

Formes disponibles: Round bars

Txoj kab uas hla: 8-60mm

Ntev: 3000mm nyob ib ncig ntawm

 

Cov tshuaj muaj pes tsawg leeg rau Stainless hlau REX 734

 

C Tsawg dua los yog sib npaug li 0,08 Mo 2 - 3
Si Tsawg dua lossis sib npaug li 0,75 Ni 9 - 11
Mn 2 - 4,25 Nb 0,25 - 0,8
P Tsawg dua lossis sib npaug li 0,025 N 0,25 - 0,5
S Tsawg dua lossis sib npaug li 0,010 Cu Tsawg dua los yog sib npaug li 0,25
Cr 19.5 Fe so

 

Mechanical zog ntawm REX-734

 

annealed specification tus nqi (bars)
tensile zog Rm Ntau dua lossis sib npaug li 740 MPa
elongation A Ntau dua lossis sib npaug li 35%
nag lossis daus hardened specification tus nqi (bars)
tensile zog Rm Ntau dua lossis sib npaug li 1060 MPa
elongation A Ntau dua lossis sib npaug li 12%

 

Lork Group yog lub ntiaj teb ua lag luam xa tawm thiab xa khoom ntawm Kev Kho Mob Qib Stainless Hlau Rex 734 (1.4472), qib siab -kev ua tau zoo alloy tshwj xeeb tsim rau kev phais, kho hniav, thiab cov cuab yeej siv kho mob. Peb cov khoom ua tau raws li cov qauv nruj thoob ntiaj teb rau biocompatibility, corrosion resistance, thiab mechanical kev ncaj ncees, ua rau lawv zoo tagnrho rau cov chaw kho mob tseem ceeb.

 

Hu rau Lork Group hnub no kom tau txais cov qauv dawb thiab cov lus hais. Peb pab neeg ua haujlwm tau npaj txhij los txhawb koj qhov project specifications thiab cov khoom siv saw hlau xav tau.

 

Hu rau tam sim no

 

Cim npe nrov: REX 734,1.4472, UNS S31675, Kho Mob Qib Stainless Hlau, X4CrNiMnMo21-9-4, ASTM F1586, ISO 5832-9, High-Nitrogen Austenitic Stainless Hlau, Kho Mob Qib Stainless Hlau