Hastelloy C2000
Hastelloy C2000 tuav, cov kav dej, thiab cov xaim hluav taws xob muaj rau kev xa khoom sai; nyem daim duab hauv qab no kom paub ntau ntxiv txog cov khoom.
Paub meej
Lork Group's siab -zoo Hastelloy C-2000 (UNS N06200 / W.Nr. 2.4675) yog ntau yam npib tsib xee-chromium-molybdenum-tungsten alloy paub txog nws qhov tshwj xeeb tiv thaiv rau ntau qhov chaw oxidizing, tshwj xeeb tshaj yog nyob rau hauv cov xwm txheej.
Peb muaj nyob rau txhua lub sijhawm los muab cov lus qhia thiab cov ntaub ntawv qhov ntev -thov tiv tauj peb.
layla@lorkgroup.com | +86 199 3707 5488
Khoom Description
Lork Group's siab -zoo Hastelloy C-2000 (UNS N06200 / W.Nr. 2.4675) yog ntau yam npib tsib xee-chromium-molybdenum-tungsten alloy paub txog nws qhov tshwj xeeb tiv thaiv rau ntau qhov chaw oxidizing, tshwj xeeb tshaj yog nyob rau hauv cov xwm txheej.
Hastelloy C2000 qhov zoo tshaj plaws fabricability tso cai rau kev yooj yim tsim, vuam, thiab machining, ntxiv rau nws versatility nyob rau hauv ntau yam kev siv. Nws txoj kev ntseeg siab thiab kev tiv thaiv corrosion ua rau nws yog qhov kev xaiv zoo tshaj plaws rau cov khoom tseem ceeb hauv cov cheeb tsam tshuaj lom neeg, nrog rau cov reactors, kub exchangers, thiab piping systems.
Hastelloy C2000 muaj kev sib xyaw tshwj xeeb ntawm cov ntsiab lus, suav nrog npib tsib xee, chromium, molybdenum, thiab tooj liab, uas ua rau nws zoo heev corrosion kuj. Cov ntsiab lus siab chromium muab kev tiv thaiv rau oxidizing xov xwm, thaum lub molybdenum thiab tungsten txhim khu nws kev tiv thaiv kom tsis txhob muaj ib puag ncig. Qhov sib ntxiv ntawm tooj liab ntxiv txhim kho nws cov kev tiv thaiv corrosion hauv ntau qhov chaw.
Cov hlau no feem ntau siv rau hauv daim ntawv thov uas muaj sulfuric acid, hydrochloric acid, phosphoric acid, acetic acid, thiab lwm yam tshuaj lom neeg. Nws kuj tseem tsim nyog siv rau hauv ib puag ncig uas muaj oxidizing ntsev thiab cov kua qaub sib xyaw. Cov hlau tsis kam rau kev ntxhov siab corrosion tawg, pitting, thiab crevice corrosion ua rau nws nyiam cov khoom siv rau cov khoom tseem ceeb hauv ntau yam lag luam.
Yam khoom
Qws, Bar, Hlau thiab Forgings:ASTM B462, ASTM B472, ASTM B564, ASTM B574, ASME SB462, ASME SB472, ASME SB564, ASME SB574
Phaj, Sheet thiab Sawb:ASTM B575, ASME SB575
Tube thiab Tube:ASTM B619, ASTM B622, ASTM B626, ASME SB619, ASME SB622, ASME SB626
Vuam khoom:AWS A5.14 ERNiCrMo-17, ASME Ⅱ SFA-5.14 ERNiCrMo-17, ASME Ⅸ F-No.43
Hastelloy C2000 Tshuaj muaj pes tsawg leeg
|
Kev sib xyaw |
Cov ntsiab lus |
|
C |
Tsawg dua los yog sib npaug li 0.01 |
|
Si |
Tsawg dua los yog sib npaug li 0.08 |
|
Mn |
Tsawg dua los yog sib npaug li 0.50 |
|
P |
Tsawg dua lossis sib npaug li 0.025 |
|
S |
Tsawg dua lossis sib npaug li 0.010 |
|
Cr |
22.0-24.0 |
|
Ni |
Bal |
|
Co |
Tsawg dua lossis sib npaug li 2.0 |
|
Mo |
15.0-17.0 |
|
AI |
1.5-4.0 |
|
Cu |
0.3-1.5 |
|
Fe |
13.0-17.0 |
Hastelloy C2000 Property
|
Qhov ceev, g / cm3 |
Melting Point, degree |
Tensile zog, MPa |
Yield zog, MPa |
ELongation,% |
Hardness, HB |
|
8.50 |
1328-1358 |
760 |
363 |
64 |
– |
Daim ntawv thov Hastelloy C2000
- Cov txheej txheem tshuaj lom neeg kev lag luam reactors, kub exchangers, kab, thiab piping
- Pharmaceutical kev lag luam reactors thiab tshuab ziab khaub ncaws
- Flue gas desulfurization systems