Lork pab pawg siab - zoo}}}} chromium alloy nrog ntxiv ntawm Molybdenum thiab titanium. Nws yog hnub nyoog - ua rau muaj ntau yam ua haujlwm.
Cov khoom lag luam
Lork pab pawg siab - zoo}}}} chromium alloy nrog ntxiv ntawm Molybdenum thiab titanium. Nws yog hnub nyoog - ua rau muaj ntau yam ua haujlwm. Cov alloy tswj tau lub zog zoo thiab oxidation tiv taus ntawm qhov kub txog li ntawm 1300℃F (700 degree).
Lub alloy yog Austenitic hauv txhua tus metallurgical tej yam kev mob. Lub zog siab thiab kev ncaj ncees zoo heev ntawm incoloy A286 ua kom cov khoom siv muaj txiaj ntsig zoo rau ntau yam ntawm cov dav hlau thiab roj av tshuab. Nws kuj tseem siv rau cov ntawv thov bastener hauv kev lag luam hauv tsheb thiab manifold, raws qib siab ntawm kev kub thiab kev nyuaj siab, s thiab hauv kev lag luam offshore thiab roj av.
Tshuaj Muaj Tshuaj
|
Lub ntsiab |
Cov ntsiab lus (%) |
|
Hlau, FE |
54 |
|
Npib tsib xee, ni |
25.5 |
|
Chromium, cr |
14.8 |
|
Titanium, ti |
2.13 |
|
Molybdenum, mo |
1.30 |
|
Manganese, mn |
1.0 |
|
Silicon, si |
0.50 |
|
Vanadium, v |
0.30 |
|
Aluminium, al |
0.18 |
|
Carbon, c |
0.040 |
|
Phosphorous, p |
0.020 |
|
Sulphur, s |
0.015 |
|
Boron, b |
0.0060 |
Cov Khoom Siv Lub Cev
|
Cov Khoom Siv |
Me me |
Muaj huab tais |
|
Ceev |
7.92 g / cm3 |
0.286 lb / hauv3 |
|
Melting taw tes |
1399 degree |
2550℃f |
Cov Khoom Siv Neeg Kho Tshuab
|
Cov Khoom Siv |
Me me |
Muaj huab tais |
|
Lub zog tensile |
1035 mpa |
150100 PSI |
|
Xij Zog Zog (@Strain 0.200%) |
759 MPa |
110000 PSI |
|
Elongation thaum so |
25% |
25% |
|
Txo thaj chaw |
40% |
40% |
|
Hardness, Brinell (kwv yees los ntawm Rockwell C tus nqi rau kev kuaj Brinell nrog 3000 kg Load / 10 hli Inch lub pob) |
304 |
304 |
|
Hardness, Knoop (kwv yees los ntawm Rockwell C tus nqi) |
330 |
330 |
|
Hardness, Rockwell C |
32 |
32 |
|
Hardness, Vickers (kwv yees los ntawm Rockwell C tus nqi) |
318 |
318 |
Txias ua haujlwm
Super Alloy A-286 muaj peev xwm ua haujlwm txias txias, thiab kev kho aneal kub yog qhov kev kho mob vim tias cov khoom siv tsis zoo vim yog kev ua haujlwm txias heev. Qhov kev daws teeb meem no anneal cua sov kev kho mob yuav ua kom cov muag muag ntawm super alloy a-286.
Vuam
Cov vuam txoj kev vuam siv rau cov hlau tsis muaj zog tseem pom zoo rau Super Alloy Aloy A- 286. Thaj chaw yuav tsum welded yuav tsum huv. Tom qab kev kho cua sov los yog kub ceev lossis preheating tsis pom zoo rau cov alloy no. Zoo dua vuam cov txiaj ntsig tuaj yeem tau txais thaum no alloy yog kev daws anealed.
Kev zam
Kev zam kev hnyav thiab teeb fwm cia yog tsim rau Super Alloy A-286. Kev zam kev hnyav yog nqa tawm ntawm 1010-1204℃(1850-2200℃f) thiab teeb forging ntawm 871-1010℃(1600-1850℃f).
Luam ntawv
Cov tshuab machining yog siv los siv tshuab Super Alloy A-286. Cov txheej txheem no cuam tshuam nrog tig, khiav, thiab milling. Nyob rau hauv cov kev hloov ua haujlwm, kev siv ntawm cov ntxhib cov cuab yeej yog pom zoo rau cov nqi txiav siab.
Kev ua laus
Super Alloy A -} 286 yog thawj daws kev kho mob tshav kub kho thaum muaj 982℃(1800℃f) ua ntej kev laus. Kev laus yuav siv qhov chaw rau 16 h ntawm 718℃f) tom qab uas cov alloy no txias hauv huab cua.
Kev puas ntsoog
Super Alloy A-286 yog qhov nyuaj los ntawm cov txheej txheem ua haujlwm txias thiab kuj muaj peev xwm ua tau lub hnub nyoog tawv vim muaj cov titanium hauv no alloy.
Kev Kho Cua Sov
Super Alloy A286 yog kev daws anealed ntawm 982℃(1800 Degree F), muaj cov roj quenched, tuav rau 16 xyoo℃f), thiab thaum kawg txias rau hauv huab cua. Qhov kev kho cua sov no txhim kho lub zog ntawm super alloy a-286.
Cov Ntawv Thov
Super Alloy A-286 yog siv nyob rau hauv cov av lim dej, cov khoom siv supercharge, cov khoom siv ntse, cov khoom siv tsis sib haum, thiab cov dav hlau sib sib zog nqus.