Cov xwm txheej tam sim no ntawm Nimonic Materials Market
Koj puas tau tawm tsam xaiv ntawm Nimonic 75 thiab Nimonic 80A? Tom qab ntau qhov kev nug, koj puas tau pom tias Nimonic series alloys tsis tshua muaj nyob hauv khw? Los yog hais tias kev cai txiav txim yuav tsum tau siab dua qhov kev txiav txim kom tsawg? Cov no tsuas yog qee qhov "cov teeb meem nyuaj" uas koj yuav ntsib.
Qhov no yog vim Nimonic series alloys kuj tsis tshua muaj nyob rau hauv lub ntiaj teb no kev ua lag luam, teej tug mus rau ib tug "niche khoom." Qhov no feem ntau yog vim nws yog thawj tiam ntawm nickel-raws li superalloys, thiab tam sim no nws qhov kev ua tau zoo tshaj los ntawm cov ntaub ntawv tshiab. Nws txoj kev lag luam tau raug coj los ntawm qib siab dua xws li Inconel 718 thiab hmoov metallurgy / ib leeg siv lead ua alloys. Txawm li cas los xij, nws tseem yog feem ntau siv hauv qee yam kev siv.
Lub Lork Group muaj cov khoom lag luam ntau ntawm Nimonic series alloys thiab muaj peev xwm ua tau yooj yim. Nws kuj tseem siv cov peev txheej no rau ISO thiab CE daim ntawv pov thawj, kev txhim kho kev lag luam, thiab kev tsim cov neeg siv khoom.
Lork Group's Nimonic 75 thiab Nimonic 80A
Ntawm no peb xub muab koj cov ntaub ntawv ntawm ob kab khoom los ntawm Lork Group: Nimonic 75 thiab Nimonic 80A. Koj tuaj yeem nyem rau saib cov ncauj lus kom ntxaws lossis tiv tauj peb rau tus nqi thiab cov lus qhia tshwj xeeb.
Nimonic 75 alloy
Peb muab Nimonic 75 npib tsib xee alloy hauv daim ntawv tuav, daim hlau, raj, coils, strips, xov hlau, forgings, thiab lwm yam.
Nimonic 80A alloy
Peb muab Nimonic 80A nickel alloy rau hauv daim ntawv tuav, daim hlau, raj, coils, strips, xov hlau, forgings, thiab lwm yam.
Nimonic 75 thiab Nimonic 80A sib piv
Txhawm rau pab koj nkag siab sai, cov lus hauv qab no piv qhov sib txawv ntawm Nimonic 75 thiab Nimonic 80A:
| Yam ntxwv Dimensions | Nimonic 75 (UNS N06075) | Nimonic 80A (UNS N07080) |
| Core Positioning | Cov tshuaj muaj zog ntxiv dag zog rau npib tsib xee-chromium-raws li alloys, hais txog kev ua tau zoo thiab kev ua tiav. | nag lossis daus hardening npib tsib xee-chromium-raws li alloys, tshwj xeeb yog tsim los rau qhov kub thiab txias dua. |
| Txhim kho Mechanism | Lub hauv paus kev txhawb zog yog los ntawm kev kho cov tshuaj kho nrog cov ntsiab lus xws li chromium thiab titanium, uas ua rau muaj zog tsawg. | Tus yuam sij rau kev ua tau zoo leap yog nyob rau hauv nag lossis daus hardening los ntawm kev ntxiv txhuas thiab titanium los ua ib lub zog ntxiv (Ni₃(Al, Ti)). |
| Cov tshuaj lom neeg tseem ceeb | Nickel (Ni): ~ 76% (sib npaug) Chromium (Cr): 18-21% Titanium (Ti): 0.2-0.6% Aluminium (Al): Tsawg dua lossis sib npaug li 0.5% |
Nickel (Ni): ~ 70% (sib npaug) Chromium (Cr): 18-21% Titanium (Ti): 1.8-2.7% Aluminium (Al): 1.0-1.8% |
| Ua haujlwm kub siab tshaj plaws | ~ 800-900 degree. | ~ 815-1000℃(ntev-term/short-term). |
| Mechanical Properties | Tensile zog: ~ 690-750 MPa Ntev: ~ 20-31% |
Tensile Strength: Ntau dua lossis sib npaug ntawm 750-1000 MPa Ntev: ~ 20-30% |
| Machinability thiab Weldability | Zoo. Lub qhov rais ua haujlwm dav (1220-950 degree), weldability zoo heev, thiab yooj yim los tsim. | Tsim nyog tab sis ntau complex. Qhov rai ua haujlwm nqaim (kwv yees li 1050-1200 degree); daws kev kho mob raws li kev laus yog xav tau rau kev ua tau zoo. |
Cov lus pom zoo rau kev yuav khoom thiab xaiv
- Xaiv NIMONIC 75 yog tias:koj cov khoom xav tau kev ua tau zoo tag nrho, ua haujlwm ntawm qhov kub qis dua 800 degree, thiab muaj cov kev xav tau siab rau cov nqi tsim khoom thiab yooj yim ntawm machining / vuam. Piv txwv suav nrog cov tais zaub mov, cov khoom siv kho mob, thiab siab - qhov kub thiab txias rau cov cua sov.
- Xaiv NIMONIC 80A yog tias:koj cov khoom yog qhov tseem ceeb kub-qhov kawg, ua haujlwm ntawm qhov kub siab tshaj 800 degree, thiab tiv taus kev ntxhov siab, qhov ua tau zoo thiab kev ntseeg siab yog qhov tseem ceeb. Piv txwv xws li turbine blades thiab turbine disks rau aero- cav lossis siab - roj turbines.
Feem ntau, qhov kev xaiv ntawm cov khoom nyob ntawm koj qhov kev lag luam -offs hais txog qhov kub thiab txias, lub zog, tus nqi, thiab kev ua haujlwm nyuaj. Yog tias koj tuaj yeem muab qhov tshwj xeeb ntawm kev ua haujlwm kub, kev ntxhov siab, thiab kev siv nyiaj ntau ntawm lub hom phiaj, peb tuaj yeem muab koj nrog kev tshuaj xyuas ntau dua.
Yuav koom tes nrog peb li cas?
Yog tias koj xav paub ntau ntxiv txog qhov chaw tshwj xeeb ntawm cov khoom lossis xav tau cov khoom lag luam customized, tau txais cov lus qhia ceev, thiab lwm yam, thov hu rau peb!