Lork Group ua tiav xa MP35N Order rau UK
Thaum lub Cuaj Hlis 2026, Lork Group ua tiav kev tsim khoom thiab tshuaj xyuas ib pawg ntawm MP35N cobalt-raws li alloy tuav, uas tam sim no tau raug xa mus rau UK cov neeg siv khoom. Tsim los ntawm kev ua haujlwm txias- kev ua haujlwm thiab kev laus thiab nrog rau SGS thib peb- tsab ntawv ceeb toom kev soj ntsuam, cov kab no yog lub hom phiaj rau kev tsim cov tshuab aerospace. Qhov kev ua tiav no ua pov thawj ntxiv thoob ntiaj teb kev lees paub ntawm lub tuam txhab kev muaj peev xwm hauv kev ua haujlwm siab -kawg tshwj xeeb alloy cov ntaub ntawv.
Raws li lub ntiaj teb loj hub rau aerospace manufacturing, lub UK imposes tsis tshua muaj nruj qauv hais txog lub zog, qaug zog kev ua tau zoo, thiab batch sib xws ntawm tshwj xeeb alloy cov ntaub ntawv. Ua tsaug rau nws lub zog ultra-siab zog, zoo heev qaug zog tsis kam, thiab superior corrosion kuj, MP35N alloy ua cov khoom tseem ceeb rau siab - lub zog aerospace cav fasteners, tsaws iav pins, thiab davhlau tswj actuator Cheebtsam. Cov neeg siv khoom hauv tebchaws Askiv koom nrog kev koom tes no yog lub chaw tsim khoom hauv zos muaj npe nrov ntawm cov khoom siv dav hlau, nrog rau cov khoom siv hauv cov dav hlau dav hlau. Qhov kev xa tawm mus rau UK sawv cev rau lwm qhov kev ua tiav tseem ceeb rau lub tuam txhab nyob rau hauv siab -kawg aerospace cov ntaub ntawv sector, tom qab nws txoj kev vam meej hauv kev lag luam hauv teb chaws Europe.
Zaub ntawm Sample Order Photos
Dab Neeg Zoo

"Golden Diameter"
A 10 mm txoj kab uas hla yog ib qho kev qhia ntau heev rau aerospace fasteners thiab precision ncej Cheebtsam. Rau MP35N ntawm txoj kab uas hla no, txias - kev ua haujlwm ntxiv yog qhov yooj yim tshaj plaws los tswj vim tias qhov deformation thaum lub caij txias yog qhov sib xws.
Ntev tswj
Qhov ntev yog feem ntau txiav txim siab kom haum rau CNC tig lossis sib tsoo ua haujlwm. Rau cov khoom xws li pins thiab bushings siv nyob rau hauv tsaws iav, raw khoom ntev feem ntau ntog nyob rau hauv no ntau yam, ua kom tiav ntawm ntau yam machining cov kauj ruam nyob rau hauv ib qho kev teeb tsa.


Kev siv tshuab
Lub zog ntawm MP35N yog nyob ntawm qhov℃ntawm kev ua haujlwm txias deformation; Feem ntau, qhov me me ntawm txoj kab uas hla, qhov siab dua qhov txias -txoj kev txo qis uas tuaj yeem ua tiav. Nyob rau hauv qhov txias - ua haujlwm thiab hnub nyoog, cov khoom tuaj yeem ua tiav lub zog tensile tshaj 1790 MPa thiab lub zog tawm los tshaj 1580 MPa.
Kev tshuaj ntsuam xyuas
Tag nrho - kev tshuaj xyuas cov ntsiab lus ntawm spectrometer paub meej tias cov tshuaj muaj pes tsawg leeg ua raws li cov qauv kev cai; cov ntsiab lus tseem ceeb-xws li Ni, Co, Cr, thiab Mo- nrog rau cov ntsiab lus impurity tag nrho poob rau hauv qhov kev teev tseg, yog li ua kom muaj kev ruaj ntseg thiab sib xws ntawm cov khoom siv los ntawm cov khoom siv raw.

MP35N-Aerospace- Cov Khoom Siv Tshwj Xeeb Qib
Tsim los ntawm SPS Technologies-US chaw tsim tshuaj paus ntawm aerospace fasteners-MP35N yog aerospace- qib tshwj xeeb cov ntaub ntawv uas muab cov kev daws teeb meem zoo rau qhov tsis sib haum xeeb xav tau ntawm lub zog, toughness, thiab corrosion kuj. Vim nws lub zog ultra-siab zog, tshwj xeeb qaug zog tiv thaiv, thiab corrosion kuj, nws ua hauj lwm raws li ib tug tseem ceeb cov ntaub ntawv rau siab - lub zog fasteners nyob rau hauv aircraft engine, tsaws iav pins, thiab ya davhlau tswj actuator Cheebtsam.
Lork Group muab cov khoom siv MP35N, muab ntau hom ntawv-xws li tuav, phaj, thiab tubing, nrog rau cov ntaub ntawv tsim nyog rau kev cog qoob loo kho mob- kom tau raws li koj cov kev xav tau tshwj xeeb. Thov nyem rau ntawm cov duab lossis cov ntawv hauv qab no kom pom cov ncauj lus kom ntxaws txog cov khoom.
Lork Group qhov kev tsim khoom muaj peev xwm
MP35N yog lub npe hu ua "ib qho nyuaj tshaj plaws-rau- tshuab superalloys"; cov kev cov nyom uas muaj nyob rau hauv nws cov txheej txheem ua rau tag nrho cov workflow-los ntawm txias txias thiab aging mus rau zaum kawg machining- muab tshwj xeeb xav kom nruj rau cov txheej txheem tswj.

Ua haujlwm txias:
Kev ua haujlwm - hardening tus nqi ntawm MP35N yog kwv yees li ob mus rau peb npaug ntawm 304 stainless hlau. Tus nqi txo ib daim duab hla yuav tsum nruj me ntsis tswj ntawm 10% thiab 15%, thiab lub tshuab nqus tsev tov annealing yuav tsum tau rov qab ductility thaum lub cumulative deformation mus txog 60% -70%. Ib txoj kab uas hla ntawm 10 hli ntog nyob rau hauv qhov "qab zib qhov chaw" rau qhov txias- txheej txheem kos duab, kom ntseeg tau tias tsis sib xws deformation thiab lub zog zoo ib yam.

Kev laus kho mob:
Kev laus kev kho mob yog cov kauj ruam tseem ceeb rau "kaw hauv" cov khoom siv lub zog. Kev laus kub yog feem ntau tswj ntawm 538℃thiab 650℃thiab yuav tsum tau ua nyob rau hauv lub tshuab nqus tsev lossis inert gas cua; Qhov kub sib txawv ntawm tsuas yog ± 15℃tuaj yeem ua rau lub zog hloov pauv ntau dua 100 MPa.

Machining:
Tom qab kev laus, MP35N nce mus txog qhov nyuaj ntawm HRC 45-52, ua rau nws yuav luag tsis tuaj yeem txiav nrog cov cuab yeej carbide zoo ib yam; yog li ntawd, roughing thiab semi- ua tiav cov haujlwm yuav tsum tau ua thaum cov khoom nyob rau hauv cov tshuaj-annealed xeev.
Kev xeem SGS
Lub tuam txhab siv kev tswj hwm zoo rau MP35N bar Tshuag, tsim kom muaj cov ntaub ntawv zoo tshaj plaws rau txhua theem los ntawm cov khoom siv raw mus rau kev xa khoom ntawm cov khoom tiav. Cov batch no tau ua tiav dhau SGS kev sim, npog qhov tseem ceeb tsis xws li tshuaj lom neeg muaj pes tsawg leeg, cov khoom siv kho tshuab, thiab tsis yog - kuaj kev puas tsuaj. Raws li tus thawj coj thoob ntiaj teb hauv kev tshuaj xyuas, kev tshuaj xyuas, kev sim, thiab ntawv pov thawj, SGS cov ntaub ntawv tshaj tawm uas tau lees paub thoob plaws hauv cov khoom siv dav hlau. Dhau qhov kev xeem SGS no tsis yog tsuas yog lees paub tias cov khoom ua tau raws li cov qauv hauv aerospace tab sis kuj muab kev tso cai thib peb - tog validation rau cov txheej txheem txais khoom ntawm UK aerospace cov neeg siv khoom.
Ib daim ntawv tshaj tawm SGS thib peb - tog neeg xeem tau suav nrog hauv cov ntawv txuas rau peb cov xov xwm hloov tshiab; koj tuaj yeem rub tawm thiab saib nws yog tias xav tau.
Vim li cas thiaj li precision manufacturing yuav tsum?

Landing gear actuator pins thiab servo valve springs yog cov khoom siv dav hlau uas tau ua ib txhij rau kev sib hloov siab heev thiab qhov chaw corrosive. Lawv thov qhov tshwj xeeb qhov tseeb qhov tseeb thiab qhov tseeb ntawm qhov chaw; thaum ib txwm muaj siab - lub zog steels muaj lub zog txaus, lawv raug rau hydrogen embrittlement. Hauv qhov sib piv, MP35N ua haujlwm zoo tshaj plaws ua tsaug rau nws qhov tshwj xeeb tsis kam rau ob qho tib si hydrogen embrittlement thiab kev ntxhov siab corrosion tawg. Tsis tas li ntawd, muab qhov sib thooj ntawm precision navigation thiab sensing cov cuab yeej rau lub tsaws iav, MP35N tsis yog - cov khoom sib nqus (magnetic permeability<1.001) prevent interference with onboard electronic systems. Ultimately, the effort invested in these demanding manufacturing processes ensures zero-failure performance of the landing gear under extreme operating conditions.
Qhov tseeb vim tias kev ua haujlwm nyuaj heev, lub peev xwm ua kom tsis tu ncua me me - txoj kab uas hla, siab - qhov tseeb MP35N tuav hauv cov neeg laus ua haujlwm ua pov thawj rau Lork Group lub peev xwm muaj peev xwm nyob rau hauv txias -txoj kev tswj, kev laus lub qhov cub kub sib xws, thiab kev sib tsoo precision.
Peb zoo siab tos txais cov lus nug los ntawm cov neeg siv khoom los tshawb nrhiav cov hauv kev rau kev sib koom tes txog kev xaiv cov khoom siv, kev ua raws cai, thiab kev sib koom tes. Tsiv mus tom ntej, lub tuam txhab yuav txuas ntxiv ua kom nws muaj nyob rau hauv siab -kawg daim ntawv thov kev lag luam, muab cov neeg siv khoom thoob ntiaj teb nrog cov txheej txheem tshwj xeeb ntawm cov khoom siv alloy zoo tshaj.