Vicalloy I Yeeb Nkab Thiab Tube Manufacturing: Extrusion, Kos duab thiab kho cua sov

Sep 28, 2026

Tso lus

Vicalloy I yog nag lossis daus-cov cobalt hardening-raws li cov hlau nplaum ruaj khov raws li Fe-Co-V system. Tsis zoo li ntau cov khoom siv hlau nplaum ruaj khov uas nyuaj rau kev tsim tom qab casting, Vicalloy I muab cov khoom sib nqus nrog cov ductility zoo nyob rau hauv cov kev daws teeb meem - kho mob, tso cai rau cov khoom siv los ua haujlwm kub, kos duab txias, dov, machining, thiab lwm yam kev ua haujlwm ua ntej kev laus kawg. Qhov "daim ntawv ua ntej, tawv tom qab" tus yam ntxwv ua rau kev tswj xyuas tshwj xeeb yog qhov tseem ceeb thaum tsim cov raj precision thiab hollow Cheebtsam.

 

Rau Vicalloy I cov yeeb nkab thiab raj tsim, cov theem tseem ceeb feem ntau muaj xws li kev npaj billet, kub ua hauj lwm los yog extrusion, txias kos duab, nruab nrab kub kev kho mob thaum xav tau, zaum kawg sizing thiab aging kev kho mob. Lub hom phiaj tsis yog kom ua tiav qhov tseeb qhov tseeb, tab sis tsim kom muaj kev sib raug zoo ntawm kev deformation, microstructure thiab cov khoom sib nqus zaum kawg.

 

Vicalloy I Cov yam ntxwv ntawm cov khoom

 

Vicalloy I belongs rau Fe-Co-V alloy system; Nws feem ntau muaj kwv yees li 50% cobalt thiab 10% vanadium, nrog rau cov seem uas feem ntau yog hlau.

 

Cov khoom sib nqus mus tas li ntawm Vicalloy I feem ntau ua tiav los ntawm kev kho cua sov. Nrog rau kev kho cua sov kom tsim nyog, Vicalloy Kuv tuaj yeem ua tau lub zog siab tshaj plaws ntawm kwv yees li 1 MGOe yam tsis tas yuav muaj qhov txias deformation. Thaum cov khoom siv hluav taws xob tuaj yeem txhim kho ntxiv los ntawm qib siab dua ntawm kev ua haujlwm txias, xws li kev ua haujlwm siab - deformation feem ntau siv rau Vicalloy II thiab nplua - cov khoom siv hlau.

 

Cov yam ntxwv no yog qhov tseem ceeb rau kev tsim tubing. Thaum lub sij hawm tsim khoom, tus nqi ntawm kev ua hauj lwm txias tsis tuaj yeem nce mus tas li tsuas yog txhawm rau txhawb zog los yog cov khoom sib nqus; Hloov chaw, cov txheej txheem deformation yuav tsum tsim kom muaj kev sib haum xeeb raws li qhov yuav tsum tau ua rau lub raj qhov kawg qhov ntev, cov khoom siv kho tshuab, thiab kev ua haujlwm sib nqus.

 

Extrusion txheej txheem

 

Vicalloy I tubing feem ntau extruded nyob rau hauv lub kub - ua hauj lwm lub xeev. Thaum ingots ntawm cov hlau no tuaj yeem tawg los ntawm kub forging lossis kub dov, extrusion yog qhov tseem ceeb hauv kev tsim cov raj xa hluav taws xob nws tus kheej.

 

Lub qhov rais extrusion kub rau Vicalloy kuv yuav tsum sib npaug ob lub hom phiaj: ua kom muaj cov yas txaus rau kev ua kom tsis zoo thaum tsis txhob muaj qhov kub thiab txias uas tuaj yeem ua rau cov nplej coarsening thiab cuam tshuam rau kev ua haujlwm uas yuav tsum tau ua rau kev kos duab txias tom ntej. Raws li cov alloy kub- cov yam ntxwv ua haujlwm, extrusion feem ntau ua nyob rau hauv qhov kub thiab txias, nrog rau cov chaw tshwj xeeb optimized raws li billet qhov ntev thiab qhov sib piv extrusion.

 

Extrusion pab tsis tau tsuas yog los tsim cov khoom, tab sis kuj los tsim lub microstructural foundation rau tom qab txias txias. Lub extruded billet yuav tsum muaj ib tug zoo li grain qauv thiab zoo nto zoo kom tiv taus qhov tseem ceeb deformation koom nrog hauv kev kos duab txias. Kev tswj tsis zoo ntawm extrusion kub tuaj yeem ua rau cov kab nrib pleb los yog microstructural inhomogeneity, ncaj qha ua rau tsis ua hauj lwm thaum lub sij hawm tom qab kos duab.
Xa tawm tswv yim

Extrusion process

 

Txias- txheej txheem kos duab

 

Drawing process

Kev kos duab yog cov txheej txheem tseem ceeb rau kev ua tiav qhov kawg qhov tseeb ntawm Vicalloy I tubing. Hauv nws txoj kev daws teeb meem -kho lub xeev, cov hlau ua pov thawj zoo plasticity, ua rau nws tsim nyog rau kev kos duab txias.

 

Kev kos duab txias ntawm Vicalloy I tubing feem ntau xav tau ntau qhov kev hla, nrog kev tswj xyuas meej ntawm thaj chaw txo tus nqi ntawm txhua theem. Kev kos duab los ntawm kev paub nrog txias- ua haujlwm Vicalloy I xaim thiab pas nrig, qhov txo qis ntawm ib qho kev hla yog khaws cia nyob rau hauv ib qho kev tsim nyog los tiv thaiv tubing pob txha los ntawm kev ua hauj lwm hnyav heev. Rau me me - txoj kab uas hla (piv txwv li, nrog ib txoj kab uas hla sab nraud tsawg dua 10 mm), mandrel daim duab yuav tsum tau tswj lub puab txoj kab uas hla, qhov loj dua tubing tuaj yeem ua tiav los ntawm hollow kos duab lossis ntsaws daim duab.

 

Vicalloy kuv tau ua haujlwm tseem ceeb thaum lub sijhawm ua haujlwm txias. Cov ntaub ntawv qhia tias alloy lub zog tuaj yeem nce los ntawm kwv yees li 530-620 MPa hauv cov tshuaj -kho lub xeev mus rau 1200-1480 MPa tom qab kos duab txias. Yog li ntawd, qhov nruab nrab annealing yog qhov tseem ceeb thaum lub sij hawm kev kos duab los kho cov yas; txwv tsis pub, cov tubing yuav tsum tau tawg thaum lub sij hawm dhau mus. Qhov nruab nrab annealing kub yog txiav txim siab raws li qhov sib txawv deformation thiab feem ntau yog teem rau hauv qab ntawm cov tshuaj kho kub.

 

Kev kho cua sov txheej txheem

 

Kev kho cua sov ntawm Vicalloy I tubing muaj ob theem -kev kho kev daws teeb meem thiab kev laus kev kho mob-txhua lub hom phiaj sib txawv ntsig txog cov txheej txheem ua tiav.

 

1. Kev kho mob

Lub hom phiaj ntawm kev kho kev daws teeb meem yog kom yaj tag nrho cov ntsiab lus alloying los ua ib qho kev daws teeb meem zoo tshaj plaws supersaturated, thaum muab kev pom zoo plasticity rau cov khoom siv los pab txhawb kev tsim tom ntej. Raws li cov ntaub ntawv muaj, kev daws teeb meem rau Vicalloy I suav nrog dej quenching los ntawm kwv yees li 1050-1100℃lossis roj quenching los ntawm ib ncig ntawm 1200 degree. Cov txheej txheem no tawm ntawm cov khoom hauv lub xeev mos-tus yam ntxwv los ntawm lub zog tensile ntawm kwv yees li 530-620 MPa thiab elongation ntawm Ntau dua lossis sib npaug li 15%- ua rau nws haum rau kev kos duab txias thiab machining.

 

2. Kev kho mob laus

Kev laus kev kho mob yog cov kauj ruam tseem ceeb rau kev tsim cov khoom sib nqus mus tas li hauv Vicalloy I tubing. Tuav cov khoom ntawm qhov kub ntawm 600℃thiab 700℃rau 2 mus rau 6 teev induces nag lossis daus ntawm vanadium- nplua nuj theem thib ob thiab kev txiav txim ntawm -theem, ua rau cov hlau nplaum tawv.

 

Pact of Aging on Tubing Properties:

  • Magnetic Properties: Coercivity nce mus rau 14.32-18.30 kA / m, remanence yog kwv yees li 0.9-1.2 T, thiab hysteresis poob ntau dua lossis sib npaug li 30 kJ / m³.
  • Mechanical Properties: Hardness nce mus rau HRC 33-40, thiab tensile zog mus txog 1200-1480 MPa.
  • Kev txwv kev ua haujlwm: Tom qab- laus, cov khoom siv nyuaj heev; tsuas yog kev sib tsoo yog ua tau, thaum cov yas sib sau los yog cov pa txiav tsis tuaj yeem ua tau.

 

Cov yam ntxwv sib nqus hysteresis ntawm Vicalloy kuv yog qhov nkag siab zoo rau qhov kub ntawm qhov kev laus, ua rau lub qhov rais nqaim. Cov kub uas qis dhau ua rau cov nag lossis daus tsis tiav thiab cov khoom sib nqus tsis txaus, thaum qhov kub siab dhau ua rau coarsening ntawm cov theem precipitated, qhov ua tau degrading hlau nplaum. Rau cov khoom siv tubing, lub sijhawm tuav tuaj yeem raug txo kom tsim nyog vim yog cov phab ntsa nyias nyias, muab qhov ntsuas kub sib xws ntawm cov phab ntsa sab hauv thiab sab nrauv.

 

Kev Tswj Xyuas Zoo ntawm Vicalloy I Tubing

 

Kev tswj kev ua tau zoo rau kev txiav txim siab Vicalloy I tubing encompasses tsis yog cov qauv ntsuas qhov ntev xwb tab sis kuj tseem saib xyuas cov khoom sib nqus, suav nrog cov yam ntxwv tshwj xeeb ntawm cov hlau nplaum ruaj khov.

 

Dimensional soj ntsuam feem ntau npog cov tsis xws li cov kab uas hla, puab txoj kab uas hla, phab ntsa thickness, ovality, ncaj, thiab nto zoo. Rau cov tubing npaj rau cov khoom sib nqus, kev sim ntxiv -xws li hardness, tensile lub zog, yield zog, thiab cov khoom sib nqus cov khoom tsis sib xws - tuaj yeem ua tau raws li cov neeg siv khoom tshwj xeeb.

 

Nto zoo kuj tseem ceeb heev. Cov teeb meem xws li khawb, kos cov cim, folds, thiab qhov chaw deformation- uas tuaj yeem tshwm sim thaum txheej txheem kos duab - tuaj yeem cuam tshuam rau kev sib dhos thiab kev ua haujlwm hauv cov khoom siv hluav taws xob zoo.

Dimensional inspection

Rau kev txiav txim kev cai, Lork tuaj yeem ua raws cov kev qhia tshwj xeeb- suav nrog qhov ntev, qhov ntev, qhov ntev, kev xa khoom, kev kho cua sov, thiab cov khoom siv tshuab thiab sib nqus- nrog rau cov neeg siv khoom. Cov Ntawv Pov Thawj Kev Xeem Khoom (MTC) thiab cov ntaub ntawv tshuaj xyuas kuj tuaj yeem muab tau raws li kev pom zoo sib koom.

 

Vim li cas Vicalloy kuv thiaj haum rau Precision Sib Nqus Cheebtsam

 

Ib tug yam ntxwv tseem ceeb ntawm Vicalloy I yog tias nws muab cov formability ua ntej kev laus kho nrog cov khoom sib nqus mus tas li ua tiav tom qab kev kho cua sov.

 

Cov yam ntxwv ntawm cov khoom no tso cai rau cov tuam txhab ua kom tiav cov txheej txheem, machining, thiab kev tswj qhov loj ntawm txoj kev nyuaj lossis siab - qhov tseeb ua ntej, thiab tom qab ntawd tau txais cov khoom sib nqus uas yuav tsum tau ua los ntawm kev kho cov laus zaum kawg. Cov ntaub ntawv keeb kwm ASM alloy piav qhia txog Vicalloy I raws li nag lossis daus -cov cobalt hardening-raws li cov hlau nplaum uas nthuav tawm cov khoom sib nqus mus tas li thaum tuav cov khoom zoo.

 

Rau cov khoom siv tubular, qhov kev ua ntu zus no - ua ntej, ua raws li cov khoom sib nqus ua kom zoo dua qub - muab cov txiaj ntsig zoo sib xws, tso cai rau kev ua tiav qhov loj me thiab cov cuab yeej sib nqus zaum kawg yuav raug kho raws li kev sib txuas tsis tau muaj kev ywj pheej ntau lawm theem.

 

Lork Vicalloy I Tubing Manufacturing

 

Lork muab Vicalloy I cov khoom hauv ntau hom ntawv kom tau raws li cov kev xav tau tshwj xeeb thiab txhawb kev ua haujlwm. Cov ntaub ntawv khoom lag luam muaj xws li cov kab puag ncig, txias- kos hlau, txias- dov strip, thiab forgings (nias qhov txuas hauv qab no kom paub meej); rau tubing, customization tuaj yeem raug soj ntsuam raws li qhov yuav tsum tau muaj qhov ntev thiab kev ua haujlwm.

Kev npaj ntau lawm rau kev cai Vicalloy I tubing tuaj yeem ua raws li cov kev cai tshwj xeeb hais txog cov kab uas hla sab nraud, sab hauv txoj kab uas hla, phab ntsa thickness, kam rau ua, deg mob, txhua yam khoom, thiab kev ua haujlwm sib nqus. Txoj kev tsim khoom tsim nyog rau cov khoom sib nqus tshwj xeeb tuaj yeem tsim los ntawm cov txheej txheem xws li kev ua haujlwm kub lossis extrusion, precision txias kos duab, thiab tswj kev laus.

 

Rau cov neeg siv khoom tsim cov khoom sib nqus tshiab, peb xav kom meej meej txhais cov khoom kawg - siv thiab sib nqus cov khoom yuav tsum ua ua ntej ua tiav qhov txias - kos duab txo qis thiab cov txheej txheem kho cua sov. Qhov no ua kom ntseeg tau tias cov tubing tsis tsuas yog ua tiav qhov siab precision thaum ua tsis tau raws li cov qauv kev sib nqus uas xav tau rau daim ntawv thov tiag tiag.

 

 

 

Lork Group
Kev Lag Luam Kev Lag Luam

Email:claire@lorkgroup.com
WhatsApp pawg:+86 19937075488

 

 

 

 

 

 

 

Xa kev nug