Nim 263
Paub meej
Lork Group siab-zoo Nimonic 263 (UNS N07263/W.Nr. 2.4650) yog lub hnub nyoog -nickel hardenable-cobalt-chrome-molybdenum alloy uas tau tsim los kom muaj cov khoom zoo heev nyob rau hauv lub zog annealed tab sis kuj zoo heev.
Khoom Description
Lork Group siab-zoo Nimonic 263 (UNS N07263/W.Nr. 2.4650) yog lub hnub nyoog -nickel hardenable-cobalt-chrome-molybdenum alloy uas tau tsim los kom muaj cov khoom zoo heev nyob rau hauv lub zog annealed tab sis kuj zoo heev.
Nimonic 263 yog qhov yooj yim rau kev tsim lossis vuam dua li lwm cov ntaub ntawv xws li Waspaloy lossis Rene 41 thiab nthuav tawm qhov kub thiab txias nruab nrab. Alloy 263 yog nkag rau hauv qhov mob annealed thiab nws cov ductility zoo heev hauv qhov mob no ua rau nws tsim nyog rau kev sib sau txias thiab ua haujlwm kub. Alloy 263 tuaj yeem welded siv cov khoom sib xyaw ua ke hauv ob daim ntawv TIG thiab MIG.
Nimonic 263 Product Form
AMS 5872 (phaj, ntawv, thiab sawb)
AMS 5966 (hli)
Nimonic 263 Chemical Composition
|
Lub ntsiab |
Cov ntsiab lus (%) |
|
Ni |
49 |
|
Co |
19-21 |
|
Cr |
19-21 |
|
Mo |
5.60-6.10 |
|
Ti |
1.90-2.40 |
|
Fe |
0.70 |
|
Mn |
0.60 |
|
Al |
0.60 |
|
Si |
0.40 |
|
Cu |
0.20 |
|
C |
0.040 - 0.080 |
|
B |
0.0050 |
|
S |
0.0070 |
Nimonic 263 Lub cev muaj zog
|
Cov khoom |
Metric |
Imperial |
|
Qhov ntom |
8.36 g / cm³ |
0.302 lb/in³ |
|
Melting point |
1300-1355 degree |
2370-2471℃F |
Cov kev kho cua sov pom zoo rau Nimonic 263 yog raws li hauv qab no
Extruded Bar
Kev Kho Mob - 1150℃rau 1.5-2.5 teev + dej quench
Kev laus kev kho mob - 800℃rau 8 teev + cua txias
(Raws li BS HR10 / AMS 5886)
Kub-rolled Sheet
Kev Kho Mob - 1150℃rau 0.5 teev + dej quench lossis cua txias
Kev laus kev kho mob - 800℃rau 8 teev + cua txias
(Raws li BS HR206 / AMS 5872)
Txias -rolled Sheet
Kev Kho Mob - 1150℃rau 3-10 mins + dej quench lossis fluidized txaj quenching
Kev laus kev kho mob - 800℃rau 8 teev + cua txias
(Raws li BS HR206 / AMS 5872)
Nimonic 263 Daim ntawv thov
Nimonic 263 feem ntau yog siv rau hauv cov roj turbine kub-section Cheebtsam.