Nimonic 80A
Lork Group muaj cov tuav, daim hlau, thiab ib daim hlab. Xav paub ntau ntxiv? Nyem rau daim duab hauv qab no kom paub meej.
Paub meej
Lork Group siab- zoo Nimonic 80A (UNS N07080 / W.Nr. 2.4952, 2.4631, GH4080A) yog wrought, hnub nyoog -nickel hardenable-chromium alloy. Nws muaj zog los ntawm kev sib ntxiv ntawm titanium thiab txhuas.
Rau quotes thiab loj cov ntaub ntawv, thov hu rau:
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488
Khoom Description
Lork Group siab- zoo Nimonic 80A (UNS N07080 / W.Nr. 2.4952, 2.4631, GH4080A) yog wrought, hnub nyoog -nickel hardenable-chromium alloy. Nws muaj zog los ntawm kev sib ntxiv ntawm titanium thiab txhuas. Nws muaj qhov tensile siab thiab nkag siab{11}} cov khoom tawg ntawm qhov kub txog li 815℃(1500℃F).
Nimonic 80A muaj corrosion zoo thiab oxidation kuj. Nws yog siv rau cov pa roj-turbine Cheebtsam (cov hniav, rings, discs), bolts, raj txhawb nyob rau hauv nuclear generators, tso li qub nyob rau hauv lub combustion engine, thiab muaj ntau lwm yam offshore / marine, automotive, thiab hluav taws xob siv.
Daim ntawv khoom
Qws, Bar, Hlau thiab Forgings:ASTM B637, BS 3076 thiab HR1
Phaj, Sheet thiab Sawb:IB HR 201
Tube thiab Tube:TIAB SA 401
Nimonic 80A tshuaj muaj pes tsawg leeg
|
Lub ntsiab |
Cov ntsiab lus (%) |
|
Cr |
18-21 |
|
Fe |
3 |
|
Ti |
1.8-2.7 |
|
Al |
1-1.8 |
|
Si |
1 |
|
Mn |
1 |
|
Cu |
0.2 |
|
Co |
0.2 |
|
C |
0.1 |
|
P |
0.045 |
|
B |
0.008 |
|
Ni |
Tshuav |
Nimonic 80A Property
|
Qhov ceev, g / cm3 |
Melting Point, degree |
Tensile zog, MPa |
Yield zog, MPa |
ELongation,% |
Hardness, HRB |
|
8.19 |
1320-1365 |
1250 |
780 |
35 |
/ |
Nimonic 80A Daim Ntawv Thov
- Aerospace:Nimonic 80A yog siv nyob rau hauv aerospace engineering rau cov khoom xws li turbine blades, combustion chambers, thiab lwm yam siab -stress qhov chaw nyob rau hauv dav hlau engine. Nws muaj peev xwm tswj tau cov khoom siv kho tshuab ntawm qhov kub siab (txog 815℃lossis 1500℃F) yam tsis muaj kev poob qis hauv lub zog lossis ductility ua rau nws tseem ceeb rau kev ua kom ntseeg tau qhov kev ua tau zoo thiab kev ua haujlwm ntev nyob rau hauv cov xwm txheej hnyav.
- Gas Turbines:Nyob rau hauv cov roj turbine xyaw, Nimonic 80A yog siv nyob rau hauv lub Cheebtsam raug kub thiab kev nyuaj siab, xws li turbine discs, hniav, seals, thiab combustion chamber. Nws tiv taus oxidation thiab thermal qaug zog pab tswj lub cav efficiency thiab kev cia siab rau lub sijhawm ua haujlwm ntev.
- Muaj cua sov:Nimonic 80A kuj tseem ua haujlwm rau hauv cov ntawv siv cua sov uas tiv taus kub thiab thermal cycling yog qhov tseem ceeb. Qhov no suav nrog cov khoom siv hluav taws xob, cov khoom siv hluav taws xob kho cua sov, thiab lwm qhov chaw raug kub hnyiab thiab cov neeg kho tshuab kev ntxhov siab.
- Lwm yam kev siv:Tshaj li aerospace thiab roj turbines, Nimonic 80A pom kev siv nyob rau hauv automotive tso li qub, nuclear reactors, thiab siab - kub structural Cheebtsam uas nws ua ke ntawm siab - kub lub zog, corrosion kuj, thiab thermal stability yog qhov zoo.
Hauv kev xaus, Nimonic 80A cov khoom tshwj xeeb ua rau nws yog qhov kev xaiv zoo tshaj plaws rau cov ntawv thov uas muaj qhov kub thiab txias ib puag ncig thiab cov neeg kho tshuab siab tau ntsib, ua kom muaj kev ntseeg siab, kev ua haujlwm, thiab kev ua haujlwm ntev hauv kev siv engineering tseem ceeb.