AMS 5586 is an Aerospace Material Specification detailing requirements for Waspaloy alloy pipes, including chemical composition, mechanical properties, heat treatment, manufacturing processes, testing, and quality control.
Xa kev nug

AMS 5586 is an Aerospace Material Specification detailing requirements for Waspaloy alloy pipes, including chemical composition, mechanical properties, heat treatment, manufacturing processes, testing, and quality control.

 

Qhov kev qhia tshwj xeeb no yog muaj raws li welded thiab kos tubing thiab feem ntau nqus-induction thiab constre electrode remelted. Ams 5586 yog npaj rau cov seem uas yuav tsum muaj kev kub ntxhov thiab kev ntxhov siab tawg.

 

Ams 5586 Waspaloy Alloy Strawber superalloy uas tuaj yeem siv nyob rau ntawm cov kev siv kub, thiab nce siab txog 1600 degree f (870 degree) rau cov ntawv thov tsawg dua.

 

Kev Kho Cua Sov

 

Ams 5586 waspaloy alloy yeeb nkab kub kho yog li nram no:

Kev Kho Mob Kev Kho Mob - Tshav kub thaum 1975 degree f (1080 degree) thiab cua txias rau 4 teev kom tsim hardness ntawm {} rockwell c;

Cov Ruaj Khetilization - Refeat rau 1550 Qib F (845 degree), thiab cua txias rau 24 teev;

Hnub nyoog harden - rheat rau 1400 degree f (760 degree) thiab cua txias rau 16 teev kom ua tiav lub hardness ntawm {3}} rockwell c;

Thov nco ntsoov tias cov nplai ntawd yuav raug tsim ntawm lub sijhawm ua haujlwm ntawm kev kho cua sov hauv oxidizing cua. Txawm li cas los xij, qhov no tsis cuam tshuam rau cov khoom ntawm cov alloy thiab tuaj yeem tshem tawm los ntawm acid pickling lossis mechanically.

 

Tshuaj Muaj Tshuaj

 

Lub ntsiab

Cov ntsiab lus (%)

Npib tsib xee, ni

56

Chromium, cr

19

Cobalt, CO

13.5

Molybdenum, mo

4.30

Titanium, ti

3

Hlau, FE

Tsawg dua los yog sib npaug rau 2

Aluminium, al

1.50

Silicon, si

Tsawg dua los yog sib npaug rau 0. 15

Manganese, mn

Tsawg dua los yog sib npaug rau 0. 10

Carbon, c

0.080

Zirconium, ZR

0.050

Boron, b

0.0060

 

Cov Khoom Siv Lub Cev 

 

Cov Khoom Siv

Me me

Muaj huab tais

Ceev

8.20 g / cm3

{{0 {}}. 296 lb / hauv3

Melting point

1358 Degree

2475 Qib F

 

Cov Khoom Siv Neeg Kho Tshuab

 

Cov Khoom Siv

Me me

Muaj huab tais

Lub zog tensile

1335 MPa

193600 PSI

Yield strength (@ strain 0.200%)

910 MPa

132000 psi

Modulus ntawm elasticity (@ 20 degree)

213 GPA

30900 Ksi

Elongation thaum so (hauv 51 mm)

26.6%

26.6%

 

Welded

 

Ams 5586 tuaj yeem yooj yim welded tsuas yog nyob rau hauv cov xwm txheej ua tib zoo uas tswj tau, siv cov txheej txheem argon-arc thiab waspaloy ams 5828 cev cov hlau. Welds yuav tsum tau zam rau ib puag ncig muaj kev ntxhov siab siab.

 

Kub ua haujlwm ntawm 11586 tau ua tiav ntawm 2140-1800 degree f ({{{2} {{2}, khoov, thiab dov rau kev ua haujlwm txias.

  • Kev tsim khoom & kev ua

    Txoj kev sib sau: Feem ntau tsis yog dab tsi, los ntawm extrusion lossis teb tsaws; nyuaj vim ua haujlwm tawv.

    Kev Kho Cua Sov: Kev daws annealing ua raws los ntawm kev laus (piv txwv li, 1080 degree daws kev kho, 845 degree tshem tawm, 760 degree kev laus).

    Machining / Vuam: Yuav tsum muaj cov tswv yim tshwj xeeb kom tsis txhob muaj kev ntxhov siab; Tom qab kev kho cua sov tom qab weld yog feem ntau tsim nyog.

  • Cov Ntawv Thov

    Aerospace: dav hlau cav Cheebtsam (tso cov tshuab ntsuas hluav taws xob), roj roj.

    Lub zog: Roj turbines (lub zog hluav taws xob), cov raj roj siab siab.

  • Kev Ntsuam Xyuas & Kev Ntsuas Zoo

    Kev Kuaj Me: Tensile, tawm lub zog, elongation, thiab kev ntsuas kev cuam tshuam hauv chav / nce kub.

    NDT: Ultrasonic, idadaraphic, lossis zas kev kuaj xyuas.

    Tshuaj Ntsuam Xyuas Tshuaj: Ua raws li cov qauv AMS.

 

 

Cov txheej txheem tsim khoom

 

product-1200-682

 

Cov ntawv thov MAIN

 

product-1200-833

 

Ntim & Xa Khoom

 

product-1200-690

product-1200-1147

 

Cov Lus Nug

 

Yog tias koj muaj lwm cov lus nug, thov hu rau kuv!

 

Q: Koj puas tuaj yeem tsim Nickel Alloy tuav?

A: Yog, peb tuaj yeem tsim cov nickel alloy tuav raws li koj cov kev xav tau.

Q: Koj qhov kev txiav txim yam tsawg kawg nkaus?

A: Peb qhov kev txiav txim qis kawg nkaus yog 50 kg. Qhov loj dua, tus nqi qis.

Q: Ntev npaum li cas yog koj lub sijhawm khoom plig?

A: Feem ntau lub sijhawm xa khoom rau Tshuag yog 3 hnub, thiab customization yuav siv sijhawm 15 hnub ua haujlwm lossis ntau dua, tab sis nws tseem muaj kev xav tau lossis kev txiav txim kom muaj nuj nqis lossis kev txiav txim kom muaj nuj nqis lossis kev txiav txim kom muaj nuj nqis.

Q: Koj puas tuaj yeem muab cov qauv?

A: Rau qhov chaw me me, peb tuaj yeem muab cov qauv dawb ntawm qhov ntau thiab tsawg thiab tsawg, tab sis tus nqi thauj khoom yuav tau xauj los ntawm koj. Rau cov qauv loj, peb yuav suav nrog nws raws cov nyiaj xaj. Thov paub meej tias muaj peb lub chaw muag khoom muag rau koj cov kev xav tau.

Q: Yuav ua li cas tuaj yeem tau txais cov npe nqi?

A: Ncaj qha xa peb email nrog cov ncauj lus kom ntxaws, thiab koj yuav tau txais cov npe nqi raug nyob hauv 1 teev.

Q: Koj yuav tswj cov khoom lag luam zoo li cas?

A: Los ntawm xaiv cov ntaub ntawv raw rau kev thauj mus los ntim, txhua txoj kev tsim khoom yuav ntsuas thiab ntsuas. Tsuas yog cov khoom lag luam uas tau dhau txhua qhov kev sim tuaj yeem xa tawm rau kev xa tawm.

Q: Koj puas tuaj yeem muab cov kev pabcuam ua haujlwm?

A: Yog, peb kuj tseem muab cov kev pabcuam ua haujlwm rau peb cov neeg siv khoom. Nws yog ib qho ntawm peb lub hom phiaj los muab cov kev pabcuam tshwj xeeb xws li kev txiav dej, kev txiav laser, thiab lwm yam fab raws li kev kos duab.

 

 

 

 

Cim npe nrov: Ams 5586 Waspaloy Alloy Yeeb Nkab, Tuam Tshoj 11886 Waspaloy Alloy Yeeb Manufacturers, Hoobkas

Xa kev nug