17-4 PH Stainless hlau yeeb nkab (UNS S17400)
Lork Group yog ib tug ua lag luam thiab exporter ntawm 17-4 PH kav thiab raj. 17-4 PH yog martensitic nag lossis daus-hardening stainless hlau nrog ntxiv ntawm tooj liab (Cu), niobium (Nb), thiab tantalum (Ta). Cov qib sib xyaw ua ke siab zog thiab hardness qhov tseem ceeb nrog rau nruab nrab corrosion kuj. Kev kho cua sov sib txawv tuaj yeem ua kom zoo rau cov khoom siv kho tshuab, piv txwv li, tawm lub zog ntawm 1100 - 1300MPa.
17-4PH yeeb nkab muaj cov yam ntxwv zoo fabricating thiab tuaj yeem muaj hnub nyoog- tawv los ntawm ib qho - kauj ruam, kev kho mob qis. Nws yog cov khoom siv ntau yam siv dav hauv aerospace, tshuaj, petrochemical, khoom noj khoom haus, ntawv, thiab kev lag luam hlau dav dav.
Yam ntxwv
- Siab zog
- Hardness (txog 572℃F / 300 degree)
- Corrosion kuj
- Cov khoom siv kho tshuab tuaj yeem ua kom zoo nrog kev kho cua sov.
- Lub zog muaj zog heev txog li 1100-1300 MPa (160-190 ksi) tuaj yeem ua tiav.
Peb khaws ntau qhov ntau thiab tsawg ntawm 17-4 PH yeeb nkab hauv Tshuag. Yog tias koj muaj kev xav tau siab rau lub sijhawm xa khoom ntawm cov yeeb nkab thiab cov raj, koj tuaj yeem paub meej nrog peb thiab thov cov lus hais.susan@lorkgroup.com | +86 199 3707 5488
Specification
|
Hom |
Cold Drawn / Welded / ERW |
|
Sab Nraum Loj |
Seamless - 1/4 "NB rau 6" NB (Nominal Bore Size) |
|
Phab ntsa Thickness |
Teem caij 10 txog Teem caij 160 |
|
Ntev |
5 mus rau 7 Meters, 09 mus rau 13 Meters, Tib Random Length, Ob Chav Random Length Thiab Customize Size. |
|
Xaus |
Plain Ends / Beveled Ends |
|
Kev Xa Khoom |
Raws li Rolled, Txias Drawn, Kub Tiav, Kev Nyuaj Siab Relieved, Annealed, Hardened, Tempered |
|
Txheej |
Electropolish, Mechanical Polish, Satin Finish, Passivated |
|
Lwm Yam Kev Xeem |
NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current Test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved, thiab lwm yam. |
|
Dimension |
Tag nrho cov kav dej yog tsim thiab Tshuaj Ntsuam Xyuas / kuaj rau cov qauv ntsig txog, suav nrog ASTM thiab ASME |
|
Kev Pab Cuam Ntxiv |
Kos / Expansion / Machining / Sand Blasting / Tua Blasting / Kub Kho |
|
Ntim |
Loose / Bundle / Ntoo Pallet / Ntoo lub thawv / Plastic Cloth Wraps / Yas End Caps / Beveled Protector |
Tshuaj muaj pes tsawg leeg
|
Lub ntsiab |
Cov ntsiab lus (%) |
|
Hlau, Fe |
73 |
|
Chromium, Cr |
15.0 - 17.5 |
|
Nickel, Nia |
3.0 - 5.0 |
|
tooj, Cu |
3.0 - 5.0 |
|
Manganese, Mn |
1.0 |
|
Silicon, Sib |
1.0 |
|
Tantalum, Tau |
0.45 |
|
Niobium, Nb (Columbium, Cb) |
0.45 |
|
Nb + Ta |
0.15 - 0.45 |
|
Carbon, C |
0.070 |
|
Phosphorus, P |
0.040 |
|
Sulfur, S |
0.030 |
Lub cev muaj zog
|
Cov khoom |
Metric |
Imperial |
|
Qhov ntom |
7.75g 3 |
0.280 lb/in³ |
Mechanical Properties
|
Cov khoom |
Metric |
Imperial |
|
Shear modulus |
77.4 gvp |
11 200 ksg |
|
Elastic modulus |
190-210 GPa |
27557-30458 dr hab |
|
Poisson tus ratio |
0.27-0.30 |
0.27-0.30 |
|
Hardness, Brinell |
352 |
352 |
|
Hardness, Knoop (kwv yees los ntawm Rockwell C) |
363 |
363 |
|
Hardness, Rockwell C |
36 |
36 |
|
Hardness, Vickers (kwv yees los ntawm Rockwell C) |
349 |
349 |
Daim ntawv thov
- Aerospace - cov qauv thiab qhov chaw
- Biomedical - cov cuab yeej tes
- Kev ua tshuaj lom neeg
- Khoom noj khoom haus txheej txheem
- Rooj vag Valves
- Mechanical Cheebtsam
- Nuclear khib nyiab ua thiab khaws cia
- Roj thiab Roj Ntau Lawm - foils, helicopter lawj platforms, thiab lwm yam.
- Pulp thiab Ntawv - cov khoom siv ntawv zeb
Cim npe nrov: 17-4PH yeeb nkab, 17-4 PH Stainless hlau yeeb nkab, UNS S17400, nag lossis daus hardening stainless hlau yeeb nkab, martensitic stainless yeeb nkab, seamless yeeb nkab, welded yeeb nkab