Hastelloy C-276 Phaj (UNS N10276)
Lork Group yog ib tus neeg muag khoom txhim khu kev qha thiab xa tawm ntawm Hastelloy C276 Sheet & Phaj hauv Suav teb. Nrog rau kev tsom mus rau precision engineering thiab kev ruaj ntseg zoo, peb muab cov kev daws teeb meem txhim khu kev qha rau cov ntawv thov kev lag luam, ua kom pom kev ua haujlwm zoo thiab kav ntev.
suav hais tias yog ib qho ntawm ntau yam corrosion resistant alloys muaj, Hastelloy C276 daim ntawv qhia tau zoo heev nyob rau hauv ib tug ntau yam ntawm cov tshuaj txheej txheem ib puag ncig nrog rau cov ferric thiab cupric chlorides, kub contaminated organic thiab inorganic media, chlorine, formic thiab acetic acids, acetic anhydride, seawater, brine thiab hypochlorite thiab chloride.
Dab tsi yog cov yam ntxwv ntawm Hastelloy C276 Sheet?
- Zoo heev corrosion kuj nyob rau hauv txo ib puag ncig
- Exceptional tsis kam mus rau cov kev daws teeb meem ntawm oxidizing ntsev, xws li ferric thiab cupric chlorides
- High nickel thiab molybdenum cov ntsiab lus muab kev tiv thaiv corrosion zoo hauv kev txo qis ib puag ncig
- Cov ntsiab lus qis carbon tsawg uas txo qis cov nplej- ciam teb carbide nag lossis daus thaum lub sijhawm vuam kom muaj kev tiv thaiv corrosion hauv tshav kub- thaj chaw cuam tshuam ntawm cov pob qij txha welded
- Kev tiv thaiv corrosion hauv zos xws li pitting thiab kev ntxhov siab -corrosion cracking
- Ib qho ntawm ob peb cov ntaub ntawv los tiv thaiv corrosive los ntawm cov roj chlorine ntub dej, hypochlorite thiab chlorine dioxide.
Peb khaws ib qho kev xaiv ntawm ntau qhov ntau thiab tsawg ntawm Hastelloy C276 Sheet hauv Tshuag. Yog tias koj muaj kev xav tau siab rau lub sijhawm xa khoom ntawm daim hlau, koj tuaj yeem paub meej nrog peb.
Specification
|
Qhov Loj: |
EN, DIN, JIS, ASTM, BS, ASME, AISI |
|
Dav: |
1000MM txog 2500MM |
|
tuab: |
0.5MM rau 200MM |
|
Ntev: |
100MM txog 600MM |
|
Daim ntawv: |
Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Checkered Phaj, Sawb, Flats, Blank (Vircle), Ntiv (Flange) |
|
Ua tiav: |
Kub dov phaj (HR), Cold Rolled Sheet (CR), 2B, 2D, BA NO (8), SATIN (Met with Plastic Coated) |
|
Hardness: |
Mos, Hard, Ib nrab Hard, Quarter Hard, Spring Hard thiab lwm yam. |
Tshuaj muaj pes tsawg leeg
|
Element |
Cov ntsiab lus (%) |
|
Nickel, Nia |
57 |
|
Molybdenum, Mo |
15-17 |
|
Chromium, Cr |
14.5-16.5 |
|
Hlau, Fe |
4-7 |
|
Tungsten, W |
3-4.50 |
|
Cobalt, Co |
2.50 |
|
Manganese, Mn |
1 |
|
Vanadium, V |
0.35 |
|
Silicon, Sib |
0.080 |
|
Phosphorus, P |
0.025 |
|
Carbon, C |
0.010 |
|
Sulfur, S |
0.010 |
Mechanical Properties
|
Cov khoom |
Metric |
Imperial |
|
Tensile zog (@thickness 4.80-25.4 hli, 538℃/ @ tuab 0.189-1.00 nyob rau hauv, 1000℃F) |
601.2 MPa rau |
8 7200 psi |
|
Yield zog (0.2% offset, @thickness 2.40 hli, 427℃/ @ thickness 0.0945 nyob rau hauv, 801℃F) |
204.8 MPa rau |
29 700 psi |
|
Elastic Modulus (RT) |
205 GPa |
29 700 tzs |
|
Elongation ntawm tawg (hauv 50.8 hli, @thickness 1.60-4.70 hli, 204℃/ @ tuab 0.0630-0.185 hauv, 399℃F) |
56% |
56% |
|
Hardness, Rockwell B (phaj) |
87 |
87 |
Daim ntawv thov
Hastelloy C276 yog siv rau rotors, bolts, shafts, hniav thiab lwm yam khoom nyob rau hauv marine daim ntaub ntawv thiab lwm yam kev lag luam, nrog rau cov pa phem tswj; khoom noj khoom haus, pov tseg thiab chemical ua; cov ntawv ua haujlwm; thiab ntau hom nroj tsuag.
Tungsten tau ntxiv rau ntau yam npib tsib xee no -chromium- molybdenum alloy, uas tiv thaiv kev xeb, kev ntxhov siab corrosion, thiab pitting. Resistant mus rau chloride ions thiab sulfur blends, Hastelloy C276 yog zoo tagnrho rau flue gas desulfurization daim ntaub ntawv.
Cim npe nrov: Hastelloy C-276 phaj, Hastelloy C-276 phaj, ASTM B575 phaj, UNS N10276 phaj, C-276 alloy phaj