Nimonic P1111 Alloy Ntawv
Nimonic Pe11 yog ib npib tsib xee-raws li supalloy nto moo rau kev kawm kub siab-kub. Tsim rau cov ntawv thov uas xav tau lub zog thiab corrosion tsis kam raws li kev ntxhov siab thermal, nws tau siv dav hauv ib lub nkoj thiab lub hwj chim loj.
Nimonic P1111 alloy ntawv (tsis muaj npib tsib xee, thiab chromium, thiab chinebardum ua rau peb11 ob leeg nag lossis ceev faj kev daws teeb meem. Alloy PE11 is commonly used in gas turbines because of its high tensile ductility strength and because it was developed for use at 550 degree (1020 degree F).
Kev Kho Cua Sov
Nimonic Pe11 yuav tsum tau daws annealed ntawm 1021 degree (1870 degree f) rau 2 h thiab tom qab cua txias. Cov txheej txheem no tau rov ua dua ob zaug ntawm 799 degree (1470 degree f) rau 2 h thiab cua txias, thiab ntawm 699 degree (1290 degree f) rau 16 h thiab cua txias.
Tshuaj Muaj Tshuaj
|
Lub ntsiab |
Cov ntsiab lus (%) |
|
Npib tsib xee, ni |
37-41 |
|
Hlau, FE |
32 |
|
Chromium, cr |
17-19 |
|
Molybdenum, mo |
4.75-5.75 |
|
Titanium, ti |
2.20-2.50 |
|
Cobalt, CO |
1 |
|
Aluminium, al |
0.70-1.0 |
|
Silicon, si |
0.50 |
|
Tooj liab, cu |
0.50 |
|
Manganese, mn |
0.20 |
|
Carbon, c |
0.030-0.080 |
|
Zirconium, ZR |
0.020-0.050 |
|
Sulphur, s |
0.015 |
|
Boron, b |
0.0010 |
Cov Khoom Siv Lub Cev
|
Cov Khoom Siv |
Me me |
Muaj huab tais |
|
Ceev |
8.02 g / cm³ |
{{0 {}}. 290 lb / nyob hauv |
|
Melting taw tes |
1280-1350 degree |
2340-2460 degree f |
Cov Khoom Siv Neeg Kho Tshuab
|
Cov Khoom Siv |
Me me |
Muaj huab tais |
|
Tensile lub zog (nag tes nyuaj, muaj nuj nqis ntawm chav tsev kub) |
1060 MPa |
154000 psi |
|
Yield strength (@strain 0.200%, precipitation hardened, value at room temperature) |
700 MPa |
102000 psi |
|
Elongation thaum so (daus daus tawv tawv) |
20% |
20% |
Thermal Khoom
|
Cov Khoom Siv |
Me me |
Muaj huab tais |
|
Thermal nthuav tawm coefficient (@ {0}} degree / 68-212 degree f) |
12. {{0 μm / m degree |
6.67 μin / hauv Degree F |
|
Thermal conductivity |
10.6 w / mk |
73.6 BTU hauv / hr.ft². Degree F |
-
Cov Khoom Siv Tseem Ceeb
Kev kub siab rau lub zog: khaws cia tensile / creep lub zog txog ~ 750 degree, zoo tagnrho rau lub tshuab ntsuas.
Oxidation tsis kam: chromium cov ntsiab lus tiv thaiv tawm tsam tawm tsam oxidative ib puag ncig.
Qoob nkees heev: Haum rau Cyclic Thermal Chaw thau khoom (piv txwv li, Dav Hlau Cav Xeem).
-
Cov Ntawv Thov
Aerospace: Kev sib txuas ua ke, turbine hniav, thiab tso tshuab.
Lub zog loj: cov pa tshuab nqus cov khoom siv, nuclele reactors.
Muaj: qhov kub kub ceev ceev, kev hloov cua sov.
-
Fabrication & Kev Ua
Txoj kev sib sau: Yuav tsum kub ua haujlwm (piv txwv li, dov ntawm lub siab kub) vim muaj lub zog siab ntawm chav tsev kub.
Vuam: nyuaj; Cov tswv yim xws li Tig lossis Electron Beam Vuam yuav siv, feem ntau xav tau kev kho tshav kub tom qab Weld.
Machining: nyuaj; Carbide cov cuab yeej thiab qeeb qeeb tau pom zoo.
Cov txheej txheem tsim khoom

Cov ntawv thov MAIN

Ntim & Xa Khoom


Cov Lus Nug
Yog tias koj muaj lwm cov lus nug, thov hu rau kuv!
Q: Koj puas tuaj yeem tsim Nickel Alloy tuav?
A: Yog, peb tuaj yeem tsim cov nickel alloy tuav raws li koj cov kev xav tau.
Q: Koj qhov kev txiav txim yam tsawg kawg nkaus?
A: Peb qhov kev txiav txim qis kawg nkaus yog 50 kg. Qhov loj dua, tus nqi qis.
Q: Ntev npaum li cas yog koj lub sijhawm khoom plig?
A: Feem ntau lub sijhawm xa khoom rau Tshuag yog 3 hnub, thiab customization yuav siv sijhawm 15 hnub ua haujlwm lossis ntau dua, tab sis nws tseem muaj kev xav tau lossis kev txiav txim kom muaj nuj nqis lossis kev txiav txim kom muaj nuj nqis lossis kev txiav txim kom muaj nuj nqis.
Q: Koj puas tuaj yeem muab cov qauv?
A: Rau qhov chaw me me, peb tuaj yeem muab cov qauv dawb ntawm qhov ntau thiab tsawg thiab tsawg, tab sis tus nqi thauj khoom yuav tau xauj los ntawm koj. Rau cov qauv loj, peb yuav suav nrog nws raws cov nyiaj xaj. Thov paub meej tias muaj peb lub chaw muag khoom muag rau koj cov kev xav tau.
Q: Yuav ua li cas tuaj yeem tau txais cov npe nqi?
A: Ncaj qha xa peb email nrog cov ncauj lus kom ntxaws, thiab koj yuav tau txais cov npe nqi raug nyob hauv 1 teev.
Q: Koj yuav tswj cov khoom lag luam zoo li cas?
A: Los ntawm xaiv cov ntaub ntawv raw rau kev thauj mus los ntim, txhua txoj kev tsim khoom yuav ntsuas thiab ntsuas. Tsuas yog cov khoom lag luam uas tau dhau txhua qhov kev sim tuaj yeem xa tawm rau kev xa tawm.
Q: Koj puas tuaj yeem muab cov kev pabcuam ua haujlwm?
A: Yog, peb kuj tseem muab cov kev pabcuam ua haujlwm rau peb cov neeg siv khoom. Nws yog ib qho ntawm peb lub hom phiaj los muab cov kev pabcuam tshwj xeeb xws li kev txiav dej, kev txiav laser, thiab lwm yam fab raws li kev kos duab.
Cim npe nrov: Nimonic P1111 Alloy Ntawv, Tuam Tshoj Nimonic Pe11 Alloy Ntawv Ntawv Cov Chaw Tsim Tshuaj, Hoobkas