AISI 310S Stainless Hlau Sheet (UNS S31008)

AISI 310S Stainless Hlau Sheet (UNS S31008)

Lork Group yog AISI 310S daim ntawv xa khoom thiab xa tawm. Cov khoom siv yog tsim rau ntau cov txheej txheem vuam xws li arc lossis TIG vuam thiab tuaj yeem siv rau forging thiab txias sib sau.
Xa kev nug

Lork Group yog AISI 310S daim ntawv xa khoom thiab xa tawm. Cov khoom siv yog tsim rau ntau cov txheej txheem vuam xws li arc lossis TIG vuam thiab tuaj yeem siv rau forging thiab txias sib sau. Cov ntawv thov kev lag luam muaj xws li ntsuas ntsuas, kev tsim hluav taws xob, thiab kev lag luam tshuaj.

 

Cov ntaub ntawv AISI 310S yog austenitic stainless hlau, tseem hu ua 1.4845, X15CrNiSi25-21. Cov khoom yog nyob rau hauv pab pawg ntawm tshav kub-resistant chromium-nickel steels thiab yog yus muaj los ntawm nws tsis kam mus rau kub kub.

 

AISI 310S yog resistant rau scaling (nyob rau hauv cov huab cua) thiab yuav siv tau mus txog rau ib tug kub ntawm 1050℃(AISI 314 / 1.4841 yog pom zoo rau qhov kub thiab txias). Stainless hlau AISI 310S tsis sib nqus / magnetisable. Nws muaj lub zog tensile ntawm 500 - 750 N / mm², hardness Tsawg dua lossis sib npaug ntawm 192 HB, thiab qhov ceev ntawm 7.9 kg / dm³ (ntawm 20℃).

 

AISI 310S yog tsim rau ntau yam txheej txheem vuam xws li arc lossis TIG vuam thiab tuaj yeem siv rau forging thiab txias sib sau. Cov ntawv thov kev lag luam muaj xws li instrumentation, furnace build, n and the chemical industry.

 

Peb khaws ntau qhov ntau thiab tsawg ntawm AISI 310S daim ntawv hauv Tshuag. Yog tias koj muaj kev xav tau siab rau lub sijhawm xa khoom ntawm daim hlau, koj tuaj yeem paub meej nrog peb thiab thov cov lus hais.

 

Specification

 

Thickness

0.3 hli ~ 200mm

Dav

1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, thiab lwm yam

Ntev

2000mm, 2440mm, 3000mm, 5800mm, 6000mm, thiab lwm yam

Txuj

JIS, AISI, ASTM, GB, DIN, EN, thiab lwm yam

Nto

Qhov saum npoo thiab tiav ntawm stainless hlau 310s ntawv:
2B, 2D, BA, Tsis yog. 1, Tsis yog. 4, Tsis yog. 8, 8K, iav, checkered, embossed, hairline, xuab zeb
blast, Txhuam, etching, thiab lwm yam

Pob

Shrink - qhwv Carton thawv, Ntoo pallets, ntoo thawv, Ntoo crates, thiab lwm yam.
xav tau.

 

Tshuaj muaj pes tsawg leeg

 

Element

310S

Cov pa roj carbon

0.08

Chromium

24.0-26.0

Nickel

19.0-22.0

Manganese

2.00

Silicon

1.50

Phosphorus

0.045

Sulfur

0.030

 

Mechanical Properties

 

Khoom

310S

Yield zog, min. (ksi)

30

Tensile zog, min. (ksi)

75

Elongation, min. (%)

40

Hardness, max. (Rb)

95

 

Daim ntawv thov

 

  • Kilns
  • Thaum tshav kub kub Exchangers
  • Radiant Tubes
  • Muffles, retorts, annealing npog
  • Tube hangers rau roj refining thiab chav boilers
  • Coal gasifier Internal Cheebtsam
  • Saggers
  • Rauv qhov chaw, conveyor siv, rollers, qhov cub hauv ob sab phlu, kiv cua
  • Cov khoom siv ua zaub mov
  • Cryogenic cov qauv

 

 

Cim npe nrov: AISI 310S, 310S Stainless Hlau, Stainless Hlau Sheet, UNS S31008, siab kub ntawv, oxidation -cov ntawv resistant, kub resistant stainless