ASTM B575 Hastelloy C-4 Nickel Alloy Sawb
ASTM B575 Hastelloy C-4 Nickel Alloy Sawb Cov Lus Qhia
Hastelloy c- 4 yog qhov siab {{} {} {}} molybdenum {} chromium alloy. Nrog nws cov ultra - Cov pa roj carbon tsawg thiab cov khoom ua kom ruaj khov rau qhov kub thiab txias thiab kub siab dua li 1040 degree.
Tom qab kev yuav peb Astm B575 Hastelloy c- 4 npib tsib xee 4 nickel alpip sawb, qee cov neeg yuav khoom feem ntau tshuab cov khoom. Txawm li cas los xij, vim nws txoj kev nyiam ua haujlwm hnyav, Hastelloy C-4 Nickel Alloy Sawb raug pom zoo rau kev siv lub xeev annealed xeev. Siv kev txiav qis dua thiab cov nqi pub dua kom tso cai rau cov cuab yeej kom nkag hauv qab cov haujlwm-tawv tawv txheej.
Yog tias koj xav tau peb los muab cov kev daws teeb meem lossis cov ntaub ntawv, xws li qhov chaw me me ntawm cov khoom, thov hu rau peb rau cov lus hais.
ASTM B575 Hastelloy C-4 Nickel Alloy Sawb tsis
Hastelloy C-4 Nickel Alloy Tshuag
Hastelloy C-4 Nickel Alloy Sawb Raug Thiab Nqe Kev Siv Khoom
Hastelloy C-4 Nickel Alloy Sawb
Cov Haujlwm Txias:
Ua haujlwm hnyav: Hastelloy c - 4 npib tsib xee ob lub siab muaj qhov siab ua haujlwm hnyav. Yog li ntawd, thaum lub sijhawm ua xws li dhuav txias, yog tias muaj kev deformation tseem ceeb, analmediate analing tej zaum yuav tau. Yog tias muaj kev ua haujlwm txias deformation ntau dua 15%, kev kho cov tshuaj theem nrab ntawm theem ob. Thov nco ntsoov tias kev ua haujlwm txias yuav tsum tau ua hauv kev daws teeb meem hauv xeev.
Kev Kho Cua Sov:
Kev Kho Mob: Cov Qauv Kev Kho Mob Cov Kev Kho Mob Kub los ntawm 1050 Qib mus rau 1100 degree. Rau ib tug nyias -}}}}}}}}}}}}}} cua txias lossis cov pa cua txias kom ntseeg tau tias muaj kev pom zoo ntawm corrosion.
Pab Pawg Lork muaj customizedASTM B575 Hastelloy C-4 Nickel Alloy SawbCov. Muab los ntawm Lork Group yog:
1. Cov Khoom Siv: $ 25-30 / kg (MOQ 30kg), $ 20-25 / kg (100-300kg)
2. Ua: Txiav, chipping, milling, thiab lwm yam (nqe raws cov ntaub ntawv poob thiab kev ua tiav)
3. Cov ntaub ntawv kev cai {- metallurgy, cua sov, thiab lwm yam kev daws teeb meem (nqe raws li koj qhov yuav tsum tau)
Yog xav paub ntxiv, thov hu rau:
Email:susan@lorkgroup.com
Whatsapp:+86 19937075488

Cov nqi sau saum toj no yog cov nqi lag luam nruab nrab cov nqi rau cov ntaub ntawv thiab yog rau siv xwb. Txog {-} tus nqi, thov xa koj daim ntawv xaj xaj rau peb kom paub cov ntaub ntawv ntxiv!
Hastelloy C-4 Nickel Alloy Tshuaj Sib Xws
| Nyhav%% | Hastelloy C-4 |
| Mn | 1.0 |
| Cr | 14.5 - 17.5 |
| Mo | 14.0 - 17.0 |
| Ti | Tsawg dua los yog sib npaug rau 0.70 |
| Zaum fe | Tsawg dua los yog sib npaug rau 3.0 |
| Co las | Tsawg dua los yog sib npaug rau 2.0 |
| MN / Si / C / S | Ib yam |
| Ni | Tus liab |
Hastelloy C-4 Nickel Alloy Cov Khoom Siv Neeg Kho Tshuab
| Khoom | Hastelloy C-4 |
| Lub zog tensile | Ntau dua los yog sib npaug rau 650 - 690 mpa |
| Paib lub zog | Ntau dua los yog sib npaug rau 275 - 280 mpa |
| Txo thaj chaw% | Ntau dua los yog sib npaug rau 40% |
| Melting kub ntau yam | 1335 ~ 1380 Qib |
Rau ntau hastelloy C-4 npib tsib xeeCov ntsiab lus, thov hu rau peb!
Cim npe nrov: ASTM B575 Hastelloy C-4 Nickel Alloy Sawb, Tuam Tshoj ASTM B575 Hastelloy C-4 Nickel Alloy Sawb Cov Chaw Tsim Tshuaj, Hoobkas