Titanium 15-3-3-3 Alloy Sawb (Ti-15V, UNS R58153)
Khoom Taw Qhia
Ti-15-3-3-3 (UNS R58153, AMS 4914; domestic qib TB5) yog ib qho metastable beta titanium alloy nrog cov muaj pes tsawg leeg ntawm Ti-15V-3Cr-3Sn-3Al. Nws lub zog tseem ceeb tsis yog nyob rau hauv qhov tshwj xeeb tseem ceeb ntawm ib qho khoom ntiag tug, tab sis hauv nws lub peev xwm los ua ke ob qho kev tsis sib haum xeeb - "txias formability" thiab "lub zog los ntawm kev kho cua sov" - hauv ib qho khoom siv. Qhov no yog ib qho kev ua tiav tsis tshua muaj sib npaug los ntawm lwm cov titanium alloys.
Qhov tseem ceeb ntawm qhov sib txawv ntawm cov khoom no thiab TC4 nyob rau hauv qhov tseeb hais tias, tsis zoo li TC4- uas yuav tsum tau cua sov kom ua tiav formability- cov khoom no tuaj yeem raug stamped ncaj qha, khoov, thiab txias - dov ntawm chav tsev kub. Tom qab ntawd nws lub zog tau nce mus rau 1100-1300 MPa ntau yam los ntawm kev tshaj tawm -kev kho cua sov. Tsis tas li ntawd, nrog qhov ceev ntawm tsuas yog 4.78 g / cm³, nws yog ze li ntawm ib nrab hnyav li stainless hlau. Rau cov ntawv thov xws li cov tawv nqaij dav hlau, cov hlua, thiab cov hlua khi- qhov twg ob qho tib si lub teeb yuag thiab cov geometries nyuaj yuav tsum tau-Ti-15-3-3-3 tam sim no sawv ua ib qho kev daws teeb meem zoo.
Txawm li cas los xij, qhov ntsuas kub tseem ceeb yuav tsum tau sau tseg kom meej: nws qhov siab tshaj plaws ntev - lub sijhawm ua haujlwm kub feem ntau tsis tshaj 300-350℃. Tshaj li qhov pib no, nws lub zog degrades loj, ua rau nws tsis haum rau siab -kub cav Cheebtsam. Txawm li cas los xij, rau kev siv hauv cov tawv nqaij dav hlau thiab cov khoom siv dav hlau, kev ua haujlwm ntawm qhov kub qis dua 300℃yog qhov txaus.
Machining thiab Vuam
Kev kho cua sov ntawm Ti-15-3-3-3 tsis nyuaj; Txawm li cas los xij, qhov kev ua tiav ntawm kev ua haujlwm thiab kev tswj hwm ntawm qhov ntsuas yuav tsum yog qhov tseeb. Peb tuaj yeem xaus qhov no yooj yim raws li txheej txheem peb kauj ruam: "Kev daws Softening → Cold forming → Aging Strengthening."
Kauj Ruam 1: Kev Kho Mob (Key rau Softening)
Kauj Ruam 2: Cold forming (Core Advantage)
Kauj Ruam 3: Kev Kho Kev Laus (Key rau Hardening)
Vuam- Ua tau, tab sis yuav tsum tau ua tom qab-welding thaum tshav kub kub kho.
Machining- Ua tau, tab sis ua rau cov cuab yeej siv siab.
Daim ntawv ceeb toom tshwj xeeb ntawm no rau cov neeg siv khoom uas nquag yuav Ti-15-3-3-3 los ntawm Lork Group: hais txog cov lus nug uas lawv tau tsa, cov ntsiab lus tseem ceeb rau kev siv lub tshuab no yog raws li hauv qab no-siv qhov tob tob ntawm kev txiav, txo cov spindle ceev, thiab xyuas kom muaj cov khoom txias txaus. Tsis txhob ntshai txiav tob; qhov kev pheej hmoo tiag tiag nyob rau hauv kev txiav qis heev. Ib qho kev txiav ntiav ua rau kev ua haujlwm nyuaj los ntawm kev sib txhuam, ua rau cov cuab yeej hnav sai thiab cov cuab yeej tsis ua haujlwm ntxov.
Kev Siv Ncaj Ncees Hauv Txias-Kev Ua Haujlwm: Rau cov khoom siv xws li cov ntsaws ruaj ruaj thiab cov hlua khi, cov neeg siv khoom tuaj yeem ncaj qha mus yuav cov hlau lossis cov hlua khi hauv cov tshuaj - kho mob, ua cov coiling txias lossis txias stamping los tsim cov khoom, thiab tom qab ntawd ua cov txheej txheem kev laus ntawm lawv tus kheej. Xwb, qee tus neeg muag khoom muab cov khoom tiav hauv qhov "txias- ua haujlwm + hnub nyoog", tab sis cov no feem ntau hais kom tus nqi siab dua.
Yog xav paub ntxiv, thov hu rau:
Email:susan@Lorkgroup.Com
WhatsApp pawg:+86 19937075488

Tshuaj muaj pes tsawg leeg
(Ti-15-3-3-3 / THIAB R58153)
| keeb | Cov ntsiab lus ntau |
| Ti | Tseem tshuav (kwv yees . 76%) |
| V | 14.0-16.0% |
| Cr | 2.5-3.5% |
| Sn | 2.5-3.5% |
| AI | 2.5-3.5% |
| O | Tsawg dua lossis sib npaug li 0.13% |
| C / N / H / Fe | Cov lej; tswj nruj heev |
Mechanical Properties
(Lub xeev sib txawv ntawm Ti-15-3-3-3 sib txawv heev.)
| Kev ntsuas kev ua haujlwm | Kev daws -Kho (Soft) | Annealed | Hnub nyoog (muaj zog) |
| Kev kho cua sov | 800-820℃Kev Kho Mob + Cua Txias | 792℃+ Cua txias | Kev Kho Mob + Txias Ua Haujlwm + 510–540℃Kev laus |
| Tensile zog | 700-800 MPa | Kwv yees li 703 MPa | 1000-1300 MPa (feem ntau yog kwv yees li . 1100 MPa) |
| Yield zog | Kwv yees li . 690 MPa | Kwv yees li . 690 MPa | Tshaj 966 MPa |
| Elongation | 20-25% | Ntau dua lossis sib npaug li 12% | 8-12% |
| Hardness | Kwv yees li 30 HRC | - | 32 HRC |
| Elastic Modulus | - | 82gp ua | 82gp ua |
Kev Sib Tham Txog Kev Sib Tham Ua Ntej Tshaj Tawm
Ua ntej pib nrog kev yuav khoom ntawm Ti-15-3-3-3 sawb lossis xaim, peb yuav tsum tau qhia ntau qhov tseem ceeb thiab cov lus qhia kom paub tseeb tias peb tuaj yeem muab koj cov lus hais tiag thiab raug:
Qhov Loj:Thickness (feem ntau rau sawb: 0.1-6.35 mm), Dav, Txoj kab uas hla (rau xaim)
Daim ntawv:Sawb, Hlau, Ntawv Nyiaj, Phaj
Qhov xwm txheej:Kev daws-kho (lub xeev mos; yooj yim rau kev ua, tab sis xav kom cov neeg siv khoom ua cov kev laus tom qab) LOSSIS Hnub nyoog (siab zog; npaj siv tam sim ntawd)?
Nto tiav:Bright, Pickled, Polished
Certification Requirements:Aerospace qib yuav tsum tau ua raws li AMS cov qauv, suav nrog EN 10204 3.1 daim ntawv pov thawj tshuaj xyuas, thiab tag nrho traceability.
Cov Lus Pom Zoo rau Kev Xaiv Txoj Cai Zoo:
Yuav tsum tau ua koj tus kheej stamping / forming / txias ua hauj lwm? → Xaiv qhov kev daws teeb meem- kho (muab; yooj yim ua haujlwm nrog).
Ua tiav springs / fasteners ncaj qha? → Xaiv Hnub nyoog (lub zog siab; npaj rau kev sib dhos ncaj qha).
Puas muaj nyob rau hauv - lub peev xwm kev laus hauv tsev tom qab ua haujlwm txias? → Kev daws teeb meem - kho yog tus nqi ntau dua - kev xaiv zoo.
Nqe Reference thiab Market Trends
Ti-15-3-3-3 yog cais raws li high-end titanium alloy. Raws li kev ua lag luam tam sim no, cov khoom lag luam tus qauv yog feem ntau muaj nyob rau hauv Tshuag; Txawm li cas los xij, cov ntaub ntawv strip thiab hlau feem ntau xav tau kev tsim khoom thiab hais kom tus nqi siab dua piv rau TC4. Muaj ntau yam cuam tshuam rau tus nqi:
Vanadium Nqe: Cov hlau muaj 15% vanadium; Kev hloov pauv hauv cov nqi lag luam vanadium ncaj qha cuam tshuam cov nqi tsim khoom.
Kev ua haujlwm nyuaj: nyias strip (<0.1 mm) is significantly more expensive than thick strip; fine wire is more expensive than coarse wire.
Qhov xwm txheej: Tus mob laus yog kim dua li Kev Kho - kho mob.
Daim ntawv pov thawj yuav tsum tau: Aerospace qib (AMS- ntawv pov thawj) yog kim dua qib industrial.
Order Volume: Chav tsev nqi siab dua rau me me -batch xaj.
Tsis tas li ntawd, cov kev qhia tshwj xeeb ntawm cov strips thiab cov xov hlau muaj qhov cuam tshuam loj rau tus nqi -tshwj xeeb, cov strips nyias hauv qab 0.1 hli thiab cov xov hlau zoo hauv qab 0.5 hli koom nrog cov txheej txheem kos duab, uas ua rau muaj nqi ntau dua. Thov muab peb cov kev qhia tshwj xeeb (thickness/inch), temper/condition, thiab xav kom muaj nuj nqis kom tau txais cov lus hais.

Cim npe nrov: titanium 15-3-3-3, alloy sawb, ti-15v, uns r58153, titanium alloy,