AMS 4914 Ti-15V-3Cr-3Al-3Sn Sawb & Ntawv
AMS 4914 Ti-15V-3Cr-3Al-3Sn Sawb & Ntawv
Ti-15V-3Cr-3Al-3Sn (abbreviated li Ti-15-3 los yog 15-3-3-3) yog ib tug tshav kub-kho metastable-type titanium alloy, characterized los ntawm nws zoo heev txias formability nyob rau hauv cov tshuaj-kho lub xeev thiab siab zog tom qab laus. Nws yog tsim rau kev tsim lub teeb yuag nyias-walled structural Cheebtsam, conduits, thiab lwm yam high-strength tsim qhov chaw.
Qhov kev qhia tshwj xeeb no suav nrog titanium alloy daim hlau thiab strips nrog lub nominal thickness tsis tshaj 0.125 nti (3.18 hli).
Cov ntaub ntawv siv
| Khoom npe | Ti-15V-3Cr-3Al-3Sn Titanium Alloy Sawb & Ntawv |
| Lub Npe | Ti-15-3 / 15-3-3-3 |
| UNS | R58153 |
| Hom alloy | Tom ntej: Metastable Beta Titanium Alloy |
| Kev Xa Khoom | Kev kho cua sov |
Tshuaj muaj pes tsawg leeg
|
Lub ntsiab
|
Min | Max |
| Vanadium | 14.0 | 16.0 |
| Chromium | 2.5 | 3.5 |
| Tin | 2.5 | 3.5 |
| Aluminium | 2.5 | 3.5 |
| Hlau | -- | 0.25 |
| Oxygen | -- | 0.13 |
| Cov pa roj carbon | -- | 0.05 |
| Nitrogen | -- | 0.05 |
| Hydrogen | -- | 0.015 |
| Lwm yam Elements, txhua | -- | 0.10 |
| Lwm yam Elements, tag nrho | -- | 0.40 |
| Titanium | seem |
Tensile zog
Rau cov khoom uas muaj nominal thickness ntawm 0.125 ntiv tes (3.18 hli) thiab hauv qab no, tus nqi strain yog teem rau 0.005 nti/inch/meter (0.005 mm/mm/meter) raws li ASTM E8/E8M tus qauv, thiab tswj ntawm ± 0.002 nti/inch/meter (0.002 mm / strat.in / meter)
| Tensile zog | 102-137 ksi (703-945 MPa) |
| Yield zog (0.2% offset) | 100 rau 126 ksi (689 rau 869 MPa) |
| Elongation ntawm 2 nti (50.8 mm) | Tsawg kawg 12% |
Khoov
Rau cov khoom uas muaj nominal thickness ntawm 0.125 ntiv tes (3.18 hli) los yog tsawg dua, yuav tsum tau npaj ib qho kev kuaj nrog lub nominal dav ntawm 0.750 nti (19.06 hli) yuav tsum tau npaj, nrog nws dabtsi yog khoov axis parallel mus rau dov kev taw qhia. Cov qauv no yuav tsum tau khoov raws li qhov kev qhia khoov raws li tau hais tseg hauv ASTM E290, nrog lub kaum sab xis ntawm 105 degrees. Lub vojvoog ntawm qhov kev sib txuas ntawm qhov kev txhawb nqa yuav tsum yog tsawg kawg yog 0.010 ntiv tes (0.25 hli), thiab lub vojvoog ntawm lub siab bar yuav tsum sib npaug rau qhov khoov coefficient pom nyob rau hauv lub rooj multiplied los ntawm nominal thickness.
Tsis muaj kab nrib pleb yuav tsum tau soj ntsuam thaum cov qauv khoov tau kuaj ntawm 15x txog 25x magnification.
| Nominal Thickness, nti | Nominal Thickness, hli | Khoov Factor |
| Mus txog 0.070, incl | Mus txog 1.78, incl | 2 |
| Tshaj 0.070 txog 0.125, incl | Tshaj 1.78 txog 3.18, incl | 2.5 |
Melting Txheej Txheem & Kev Tswj Xyuas Zoo
Ti-15V-3Cr-3Al-3Sn titanium alloy yuav tsum raug tsim los ntawm ntau lub voj voog melting raws li cov khoom siv tshwj xeeb. Cov txheej txheem melting thawj zaug tuaj yeem siv tau txais kev pom zoo ntawm lub tshuab nqus tsev lossis cov khoom siv hluav taws xob tsis siv hluav taws xob, hluav taws xob hluav taws xob hluav taws xob kub kub melting, los yog plasma arc txias hearth melting. Tom qab lub voj voog melting yuav tsum tau ua siv lub tshuab nqus tsev Arc Remelting (VAR), uas tsis muaj kev sib txuas ntxiv tau tso cai thaum lub voj voog melting kawg.
Cov txheej txheem melting tswj no pab tswj cov tshuaj muaj pes tsawg leeg sib xws thiab txhawb nqa cov kev xav tau zoo ntawm cov ntawv ua haujlwm siab titanium alloy ntawv thiab sawb. Melting cov ntaub ntawv thiab cov ntaub ntawv traceability yuav tsum tau khaws cia raws li qhov yuav tsum tau ua los ntawm cov kev qhia tshwj xeeb thiab kev yuav khoom.

Lork Group
Kev Lag Luam Kev Lag Luam
Email:layla@lorkgroup.com
WhatsApp pawg:+86 199 3707 5488
Cim npe nrov: AMS 4914, Ti-15V-3Cr-3Al-3Sn strip, Ti-15-3 titanium ntawv, 15-3-3-3 titanium alloy, beta titanium, titanium alloy ntawv, txias formable titanium sawb