Hastelloy C4

Lork Group muaj ib qho - nres kev pabcuam rau Hastelloy C4 tuav, daim hlau, thiab strips. Nyem rau daim duab kom ua raws li qhov txuas kom paub ntau ntxiv txog cov khoom lag luam.

Hastelloy C4 Alloy Bar(ASTM B574)
page-600-600
UNS N0645 / Hastelloy C4 Nickel Sheet
Hastelloy C-4 Nickel Alloy Strip(ASTM B575)
page-600-600

Paub meej

 

Lork Group lub siab -zoo Hastelloy C4 (UNS N06455/W.Nr. 2.4610) yog nickel-chromium-molybdenum alloy paub txog nws qhov tshwj xeeb tiv thaiv rau ntau qhov chaw corrosive, tshwj xeeb hauv kev txo qis.

Thov hu rau peb kom paub ntau ntxiv txog tus nqi thiab qhov ntev.
📧 layla@lorkgroup.com | 📞 +86 199 3707 5488

 

Khoom Description

 

Lork Group lub siab -zoo Hastelloy C4 (UNS N06455/W.Nr. 2.4610) yog nickel-chromium-molybdenum alloy paub txog nws qhov tshwj xeeb tiv thaiv rau ntau qhov chaw corrosive, tshwj xeeb hauv kev txo qis. Cov hlau no muaj cov qib siab ntawm kev tiv thaiv kev ntxhov siab corrosion cracking, pitting, thiab crevice corrosion, ua rau nws haum rau siv nyob rau hauv nruj heev tshuaj ua ib puag ncig.

Cov ntsiab lus tseem ceeb hauv Hastelloy C4, suav nrog npib tsib xee, chromium, thiab molybdenum, pab txhawb rau nws cov khoom tiv thaiv corrosion zoo heev. Cov ntsiab lus siab chromium muab kev tiv thaiv rau oxidizing media, thaum lub molybdenum txhim kho nws cov kev tiv thaiv kom tsis txhob muaj ib puag ncig. Tsis tas li ntawd, cov ntsiab lus ntawm cov pa roj carbon tsawg hauv Hastelloy C4 txo qis carbide nag lossis daus thaum lub sij hawm vuam, ua kom cov khoom siv corrosion kuj nyob rau hauv welded mob.

 

Hastelloy C4 feem ntau yog siv rau hauv daim ntawv thov uas muaj kub, paug cov ntxhia hauv cov kua qaub, cov organic thiab inorganic chloride- cov kab mob sib kis, thiab txo qhov chaw ib puag ncig. Nws pom kev siv dav hauv kev ua tshuaj, tshwj xeeb hauv kev tsim cov chlorinated cov kuab tshuaj, rov ua dua cov roj nuclear, thiab hauv kev lag luam tshuaj thiab petrochemical. Nws tiv taus corrosion thiab muaj peev xwm tiv taus siab - kub thiab siab - cov kev kub ntxhov ua rau nws yog ib qho tseem ceeb rau cov khoom siv tseem ceeb xws li reactors, heat exchangers, thiab piping systems.

Lub alloy qhov zoo tshaj plaws fabricability tso cai rau yooj yim txoj kev, vuam, thiab machining, ntxiv rau nws versatility nyob rau hauv ntau yam kev siv. Nws txoj kev ntseeg siab thiab kev tiv thaiv corrosion ua rau nws yog qhov kev xaiv zoo tshaj plaws rau cov khoom tseem ceeb hauv cov tshuaj lom neeg nruj heev.

 

Daim ntawv khoom

 

ASTM B 574 Cov khoom lag luam

ASTM B 575 Cov Lus Qhia Tshwj Xeeb

ASTM B619 Cov khoom lag luam

ASTM B 622 Cov khoom lag luam

ASTM B626 1

TIAB SA 2.4610

 

Hastelloy C4 Chemical Composition

 

Element

Cov ntsiab lus (%)

Chromium, Cr

14-18

Molybdenum, Mo

14-17

Hlau, Fe

3 max

Cobalt, Co

2 max

Manganese, Mn

1 max

Titanium, TSI

0.7 max

Silicon, Sib

0.08 max

Phosphorus, P

0.04 max

Sulfur, S

0.03 max

Carbon, C

0.015 max

Nickel, Nia

Tseem tshuav

 

Hastelloy C4 Property

 

Cov khoom

Metric

Imperial

Tensile zog

738mpa ua

107 000 psi

Yield zog (@0.2% offset)

492 MPa ua

7 1400 psi

Elastic modulus

211 GPA

30 600 tzs

Elongation ntawm tawg (hauv 50.8 hli)

42%

42%

 

Daim ntawv thov Hastelloy C4

 

  • Cov khoom siv tshuaj ua haujlwm
  • Nuclear fuel processing
  • Kev lag luam Petrochemical
  • Kev lag luam kws tshuaj

 